Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Glastic
Trade Name Laminates/Shapes
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength.
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
ASTM D792
Water Absorption 0.25 %
0.25 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 345 MPa
50000 psi
ASTM D638
Tensile Modulus 14.0 GPa
2030 ksi
ASTM D638
Flexural Strength 552 MPa
80100 psi
ASTM D790
Flexural Modulus 21.0 GPa
3050 ksi
ASTM D790
Compressive Strength 97.0 MPa
14100 psi
Transverse; ASTM D695
276 MPa
40000 psi
Axial; ASTM D695
Shear Strength 14.0 MPa
2030 psi
In-plane. ASTM D3914
Izod Impact, Notched 21.4 J/cm
40.1 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 6.00 µm/m-°C

@Temperature 20.0 °C
3.33 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.290 W/m-K
2.01 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 155 °C
311 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Surface Resistance 8.30e+13 ohm
8.30e+13 ohm
Insulation Resistance, ASTM D257
Dielectric Constant 5.0

@Frequency 60 Hz
5.0

@Frequency 60 Hz
ASTM D150
Dielectric Strength 3.00 kV/mm
76.2 kV/in
1 in. axial in oil; ASTM D149
Arc Resistance 130 sec
130 sec
ASTM D495