Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 0.0050 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
NuSil SCV1-2596 Silicone, Ultralow Outgassing™
General Purpose: Ultralow OutgassingComments: Electrically ConductiveCure system: PlatinumInformation provided by NuSil
Volume Resistivity <= 0.0050 ohm-cm
<= 0.0050 ohm-cm
Mil G 83528
Precision Polymer Engineering S70S Conductive Silicone Rubber
Tan coloured, Silicone Rubber, 71-80 °IRHD. Electrically conductive, Silver/Aluminum filled silicone rubber.Applications: Specially compounded to offer excellent physical and electrical properties..
Volume Resistivity <= 0.0050 ohm-cm
<= 0.0050 ohm-cm
Mil-G-83528
P & P Technology EC-H Silver Copper Loaded Fluorosilicone
P & P Technology material reference EC-H is a printing grade fluorosilicone elastomer with a Silver/Copper conductive filler and is green in color. The material is specially compounded to offer exc..
Volume Resistivity <= 0.0050 ohm-cm
<= 0.0050 ohm-cm
Mil-G-83528
P & P Technology EC-H Silver Copper Loaded Silicone
P & P Technology material reference EC-H is a printing grade silicone elastomer with a Silver/Copper conductive filler and is Tan in color. The material is specially compounded to offer excellent p..
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
as supplied without pressure sensitive adhesive; MIL-DTL-83528
Parker Chomerics CHO-SEAL 1212 Conductive Elastomer
High strength, hard (80 shore A) material for waveguide, choke, cover, and flanges with grooves for EMI and pressure sealing.Molded onlyRoHS Compliant Information provided by Chomerics
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
as supplied without pressure sensitive adhesive
Parker Chomerics CHO-SEAL 1240 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
as supplied without pressure sensitive adhesive
Parker Chomerics CHO-SEAL 1278 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Volume Resistivity <= 0.0050 ohm-cm
<= 0.0050 ohm-cm
Cured; QAP-1017
Parker Chomerics Tecknit® 72-00005 Silver-Filled Flexible Resin Caulking System
Description: TECKNIT standard electrically conductive caulks consist of four one-component resin systems filled with silver plated glass or copper particles. These systems are formulated to provide ..
Volume Resistivity <= 0.0050 ohm-cm
<= 0.0050 ohm-cm
Parker Chomerics Tecknit Consil®-C 873 Silver-Copper Filled Silicone Elastomer
Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest s..
Volume Resistivity <= 0.0050 ohm-cm
<= 0.0050 ohm-cm
Parker Chomerics Tecknit Consil®-N 891 Silver-Nickel Filled Silicone Elastomer
Description: CONSIL-N is a silicone elastomer filled with silver-plated nickel particles and designed to provide high shielding effectiveness and corrosion resistance. CONSIL-N is available in sheet..
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
Parker Chomerics Tecknit Teckfip™ FIP-R Formed in Place Conductive Elastomer
Description: FIP-R is based on a very rugged pure silver particle. By using silver as the conductive medium, this compound offers great performance in terms of heat aged electrical conductive stabil..
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
NuSil CV1-2646 Silicone, Conductive/Static Dissipative
General Purpose: Two Part Adhesive and SealantCure system: AlkoxyInformation provided by NuSil
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
NuSil CV-2644 Silicone, Conductive/Static Dissipative
General Purpose: Two Part Adhesive and SealantCure system: PlatinumInformation provided by NuSil
Volume Resistivity <= 0.0050 ohm-cm

@Temperature 65.6 °C,
Time 7200 sec
<= 0.0050 ohm-cm

@Temperature 150 °F,
Time 2.00 hour
Parker Chomerics CHO-BOND 360-20 Conductive Epoxy
Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E..
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
cured 4 hours at 65°C
Resin Technology Group TIGA 908 Gold Bonder - Low Stress Silver Conductive
100 parts resin to 6 parts hardener.TIGA 908 is a low stress, conductive silver filled epoxy adhesive. It is recommended for bonding, and sealing electronic applications which require bonding to gol..
Volume Resistivity <= 0.0050 ohm-cm
<= 0.0050 ohm-cm
Sinotek Materials R20 C Carbon Rod for Dry Battery
We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof..
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
cured 5 min @ 125°C
Tra-Con Tra-Duct 2960 Snap Cure Electrically Conductive Silver-Filled Epoxy
TRA-DUCT 2960 is a one or two-part, specially refined and processed silver filled adhesive for high speed manufacturing. Recommended for the microelectronic, automotive computer and telecommunicatio..
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
cured 2 hrs @ 65°C
Tra-Con Tra-Duct 916H04 Room Temperature Cure, Conductive Silver Epoxy Adhesive
TRA-DUCT 916H04 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical pr..
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
cured 1 hr @ 70°C
Tra-Con Tra-Duct 926H01
Information provided by Tra-Con Inc.
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
Tra-Con Tra-Duct 926K01 Long Work Life Flexible Silver-Filled Epoxy Adhesive
TRA-DUCT 926K01 is recommended for electronic bonding, coating and sealing applications that require high flexibility coupled with excellent electrical and mechanical properties. This two-part epoxy..
Volume Resistivity >= 0.0050 ohm-cm
>= 0.0050 ohm-cm
Epoxy Technology EPO-TEK® 430 Epoxy
Product Description: A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding ..
Volume Resistivity >= 0.0050 ohm-cm
>= 0.0050 ohm-cm
Epoxy Technology EPO-TEK® 431 Copper Filled Epoxy
A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding and EMI RF shielding...
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
Cured property; ASTM D257
Aptek 2210A/B Electrically conductive urethane adhesive
Electrically conductive urethane adhesive, silver-filled, flexible low modulus, low outgassingAPTEK 2210-A/B is a two component, silver-filled, urethane adhesive designed for application where flexi..
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
Cured property; ASTM D257
Aptek 2312-PMF Electrically conductive, low modulus adhesive
Premixed-frozen, electrically conductive, low modulus adhesiveAPTEK 2312-PMF is a one component, premixed-frozen, silver filled, electrically conductive soft paste adhesive. It is designed to bond m..
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
Cured property; ASTM D257
Aptek 6512-PMF Electronic grade, conductive epoxy adhesive
APTEK 6512-PMF is a one component, 100% solid, silver-filled, electrically conductive epoxy adhesive specifically designed for the attachment of electronic components to printed circuit boards. APT..
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
Cured property; ASTM D257
Aptek 6516-A/B Electrically conductive epoxy adhesive
General purpose, electrically conductive epoxy adhesiveAPTEK 6516-A/B is a two component, 100% solid, silver filled electrically conductive epoxy adhesive specifically designed for the attachment of..
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
Aremco Aremco-Bond™ 616 Electrically & Thermally Conductive Adhesive, Silver-Filled
Electrically Conductive, Silver-Filled Epoxy Good Corrosion Resistance and Mechanical Strength to 360 °F Two-Part Paste
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
Chomerics MAT-1002
Parker Chomerics CHO-FORM 5528 Conductive Form-In-Place Gaskets
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..
Volume Resistivity <= 0.0050 ohm-cm
<= 0.0050 ohm-cm
QA-1039
Parker Chomerics Waveguide Gaskets 873 Conductive Silicone Elastomer Gasket
Description: TECKNIT® WAVEGUIDE GASKETS are made from a silicone elastomer filled with silver-plated particles designed to achieve maximum electrical conductivity.Application Information: TECKNIT W..
Volume Resistivity <= 0.0050 ohm-cm
<= 0.0050 ohm-cm
Sinotek Materials 3rd Class Carbon Rod for Dry Battery
We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof..