Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M VHB™ F9469PC Adhesive Transfer Tapes with Adhesive 100MP

Category Polymer , Adhesive
Manufacturer 3M
Trade Name VHB™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M VHB™ F9469PC Adhesive Transfer Tapes with Adhesive 100MP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion strength than typical pressure sensitive adhesive systems. These 3M™ VHB™ Adhesive Transfer Tapes are transparent and are ideal for use in many interior and exterior industrial applications to replace rivets, spot welds, liquid adhesives, and other permanent fasteners.Information provided by 3M
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
Thickness 102 microns
4.00 mil
Liner Material
127 microns
5.00 mil
Adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.690 MPa
100 psi
T-Block on Aluminum; ASTM D987
Shear Strength 0.552 MPa
80.0 psi
Dynamic Shear to Stainless Steel; ASTM D1002
Peel Strength 1.40 kN/m
8.00 pli
to Stainless Steel; ASTM D3330
Thermal Properties Metric English Comments
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
Thermal Conductivity 0.669 W/m-K
4.64 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 149 °C
300 °F
Long Term
260 °C
500 °F
Short Term
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+6 ohm
>= 1.00e+6 ohm
ASTM D1000
Dielectric Strength 39.4 kV/mm

@Temperature 125 °C
1000 kV/in

@Temperature 257 °F
ASTM D149-97A
39.4 kV/mm

@Temperature 175 °C
1000 kV/in

@Temperature 347 °F
ASTM D149-97A
47.2 kV/mm

@Temperature 23.0 °C
1200 kV/in

@Temperature 73.4 °F
ASTM D149-97A
74.8 kV/mm

@Temperature 175 °C
1900 kV/in

@Temperature 347 °F
ASTM D149-97A
102 kV/mm

@Temperature 125 °C
2600 kV/in

@Temperature 257 °F
ASTM D149-97A
118 kV/mm

@Temperature 23.0 °C
3000 kV/in

@Temperature 73.4 °F
ASTM D149-97A
217 kV/mm

@Temperature 23.0 °C
5500 kV/in

@Temperature 73.4 °F
ASTM D149-97A
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Liner 58# polycoated Kraft
Copyright © lookpolymers.com All Rights Reserved