| Category | Polymer , Thermoplastic , Fluoropolymer , PTFE |
| Manufacturer | Adamas |
| Trade Name | Adalon® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Adamas Adalon® 466 PTFE, Mineral/Organic Filler.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.68 - 1.70 g/cc | 1.68 - 1.70 g/cc | ASTM D792 |
| Deformation | 1.4 - 1.8 % | 1.4 - 1.8 % | ASTM D621 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 70 - 74 | 70 - 74 | ASTM D2240 |
| Ball Indentation Hardness | 110 - 150 MPa | 16000 - 21800 psi | ISO 2032 |
| Tensile Strength at Break | >= 128 MPa | >= 18600 psi | ASTM D4894 |
| Elongation at Break | >= 2.5 % | >= 2.5 % | ASTM D4894 |
| Coefficient of Friction, Dynamic | 0.19 - 0.20 | 0.19 - 0.20 | ASTM D1894 |
| Coefficient of Friction, Static | 0.21 - 0.24 | 0.21 - 0.24 | ASTM D1894 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C 177 |
| Melting Point | 327 °C | 621 °F | DSC |
| Maximum Service Temperature, Air | 230 °C | 446 °F | DSC |
| Minimum Service Temperature, Air | -80.0 °C | -112 °F | DSC |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | ASTM D257 |
| Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ASTM D257 |