Physical Properties Metric English Comments
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Ovation Polymers RIGITRON 30545 GF Polyester, 45% Glass Reinforced
Polyester – 45% Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Var..
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 4004 FR A HS Polyphthalamide (PPA), Glass Fiber - Flame Retardant - Heat Stabilized
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
RTP Company RTP 2109  Polyetherimide (PEI) Glass Fiber 50%  (discontinued **)
Glass Fiber 50%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Solvay Specialty Polymers Halar® 1450LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)
Information provided by Solvay Specialty Polymers.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Solvay Specialty Polymers Halar® 300DA Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Information provided by Solvay Specialty Polymers.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Solvay Specialty Polymers Halar® 300LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (discontinued **)
Information provided by Solvay Specialty Polymers.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Information provided by Solvay Specialty Polymers.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Information provided by Solvay Specialty Polymers.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Solvay Specialty Polymers Halar® 901 Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)<
Information provided by Solvay Specialty Polymers.
Specific Gravity 1.68 g/cc
1.68 g/cc
Kuraray Genestarâ„¢ GA2330 Nylon, 33% Glass Filled
Abrasion Resistance V-0 Grade. Can be used for applications requiring high abrasion and heat resistance, as well as flame retardancy, such as internal gear of copying machine.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP RFN169 PA 66
LNP* LUBRICOMP* RFN169 is a compound based on Nylon 66 containing 30% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant, Flame Retardant.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Techmer ES Plaslube® J-1305/30/TF/15 BK5011 PPS
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66
LNP THERMOCOMP* RF00C is a compound based on Nylon 66 resin containing 60% Glass Fiber.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Teknor Apex APEX® 65015 Polyvinyl Chloride, Flexible
Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 1307 P-1 SI Polyphenylene Sulfide (PPS), Glass Fiber - Silicone Lubricated
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 1407 N Polyethersulfone (PES), Glass Fiber - High Viscosity
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 1407 Z Polyethersulfone (PES), Glass Fiber - FDA Compliant Ingredients
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 2799 S X 118623 B Saturated Styrenic Block Copolymer, EMI/RFI Shielding
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 1305 C TFE 15 Polyphenylene Sulfide (PPS); Glass Fiber Reinforced - PTFE Lubricated
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 1307 C Polyphenylene Sulfide (PPS), Glass Fiber
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 200 TC-C-20 FR Nylon 6/6 (PA), Thermally Conductive - Electrically Conductive - Flame Retardant
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Clariant Renol PA111G60 Nylon 66, 60% Glass Fiber
Data provided by Clariant Masterbatches
Specific Gravity 1.68 g/cc
1.68 g/cc
Epoxy Technology EPO-TEK® H65-175MP Thermally Conductive Epoxy
Product Description: EPO-TEK® H65-175MP is a single component, alumina-filled epoxy for military hybrid die and component attach. It can also be used for semiconductor and high temperature ceramic ..
Specific Gravity 1.68 - 1.70 g/cc
1.68 - 1.70 g/cc
ASTM D792
Adamas Adalon® 466 PTFE, Mineral/Organic Filler
Information provided by Adamas, HPM
Specific Gravity 1.68 g/cc
1.68 g/cc
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
PolyOne Edgetek® AT-25GF-10MN/000 BLASCK Acetal-Copolymer, Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
PolyOne Edgetek® AT-25GF-10MN/000 NATURAL Acetal-Copolymer, Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
RTP Company RTP 4005.3A FR  Polyphthalamide - Hot Water Mold (PPA) Glass Fiber 33% - Flame Retardant
Glass Fiber 33% - Flame RetardantComments:Glass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information ..
Specific Gravity 1.68 g/cc
1.68 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1105-7241-1 PEEK, with glass fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.dynamic stressChemical and hydrolysis resistance pa..
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Gromax CCP PET 9130-200 30% Glass Filled
Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell..