Physical Properties Metric English Comments
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Ovation Polymers RIGITRON 30545 GF Polyester, 45% Glass Reinforced
Polyester – 45% Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Var..
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Quadrant EPP Symalit® ECTFE Ethylene-Chlorotrifluoroethylene (ASTM Product Data Sheet)
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded  (d
AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, ..
Specific Gravity 1.68 g/cc
1.68 g/cc
ISO 1183A
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded  (d
AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, ..
Specific Gravity 1.68 g/cc
1.68 g/cc
73°F; ASTM D792
Matrixx Group 84S7301 Flame Retardant 30% Glass Reinforced PET (V0)  (discontinued **)
Data provided by The Matrixx Group, formerly RePlas.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 803 TFE 20 Acetal (POM), Glass Fiber - PTFE Lubricated
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Solvay Specialty Polymers Halar® 1450LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)
Information provided by Solvay Specialty Polymers.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Information provided by Solvay Specialty Polymers.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Information provided by Solvay Specialty Polymers.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Solvay Specialty Polymers Halar® 558 Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)<
Halar 558 fluoropolymer is a resin grade for foam extrusion applications, including primary insulations, coaxial cable cores, cross-webs, fire alarm cable, jackets, and foam tubing. Like other grade..
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
PolyOne Therma-Tech™ NJC-7500 TC Nylon 12  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Specific Gravity 1.68 g/cc
1.68 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Samsung Cheil Industries Infino® XP-2150IM PPS, 50% Glass Reinforced
PPS/GS that is used in mobile phone LCD bracketInformation provided by Samsung Cheil Industries.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66
LNP THERMOCOMP* RF00C is a compound based on Nylon 66 resin containing 60% Glass Fiber.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Samsung Cheil Industries Infino® XP-2150IM PPS, 50% Glass Reinforced
PPS/GS that is used in mobile phone LCD bracketInformation provided by Samsung Cheil Industries.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Teknor Apex APEX® 65015 Polyvinyl Chloride, Flexible
Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 1099 X 52742 H Polybutylene Terephthalate (PBT), Glass Fiber - Mineral - Flame Retardant - UL94
RTP 1099 X 52742 H is a UL94 listed PBT material which has been designed to provide an optimal balance of structural and electrical properties with easy processing characteristics and excellent dim..
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 1307 D Polyphenylene Sulfide (PPS), Glass Fiber
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 1307 P-1 SI Polyphenylene Sulfide (PPS), Glass Fiber - Silicone Lubricated
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 1407 Z Polyethersulfone (PES), Glass Fiber - FDA Compliant Ingredients
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 1307 Polyphenylene Sulfide (PPS), Glass Fiber - UL94 V-0
This series of compounds offer outstanding strengths combined with good heat and chemical resistance which may successfully be maintained in low load applications operating up to 500F. These ignitio..
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 200 TC-C-20 FR Nylon 6/6 (PA), Thermally Conductive - Electrically Conductive - Flame Retardant
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D 792
RTP Company RTP 200 TC-C-25 Nylon 6/6 (PA); Thermally Conductive - Electrically Conductive
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Clariant Renol PA111G60 Nylon 66, 60% Glass Fiber
Data provided by Clariant Masterbatches
Specific Gravity 1.68 g/cc
1.68 g/cc
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
PolyOne Edgetek® AT-25GF-10MN/000 BLASCK Acetal-Copolymer, Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
PolyOne Edgetek® ATH-25GF-10MN/000 Acetal-Homopolymer, Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedChemically CoupledInformation provided by PolyOne Corporation.
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
PolyOne Therma-Tech™ ES-5500C TC-EM Polyethersulfone  (discontinued **)
Description/Features:Thermally ConductiveCeramic FilledPolyOne First ChoiceInformation provided by PolyOne Corporation.
Specific Gravity 1.68 g/cc
1.68 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1105-7241-1 PEEK, with glass fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.dynamic stressChemical and hydrolysis resistance pa..
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Solvay Specialty Polymers Amodel® AFA-4133 V0 Z Polyphthalamide (PPA), Dry  (discontinued **)
Amodel AFA-4133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..