Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 30 m²/g | 30 m²/g | Statistical thickness surface area; ASTM D 6556 |
Orion Engineered Carbons CORAX® N 772 ASTM Carbon Black Standard grade of furnace black in accordance with the requirements of ASTM D 1765Soft Black - carcass grade, semi-reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Specific Surface Area | 30 - 70 m²/g | 30 - 70 m²/g | |
American Elements Aluminum Nanoparticles General DescriptionAluminum (Al) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Aluminum Particles are typically 10-30 nanometers (nm) with sp.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Antimony Tin Oxide Nanoparticles General DescriptionAntimony Tin Oxide (ATO) Nanoparticles, nanopowder, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. N.. |
|||
Specific Surface Area | 30 - 70 m²/g | 30 - 70 m²/g | |
American Elements Beryllium Nanoparticles General DescriptionBeryllium (Be) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Beryllium Particles are typically 20-60 nanometers (nm) with specif.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Calcium Carbonate Nanoparticles General DescriptionCalcium Carbonate (CaCO3) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Carbonate Particles are typically 10 - 80 nanometers (.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Dysprosium Nanoparticles General DescriptionDysprosium (Dy) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 10 - 80 nanometers (nm) with sp.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Dysprosium Oxide Nanopowder General DescriptionDysprosium (DyO) Oxide Nanopowder or Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Oxide Particles are typically 10 -.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Erbium Nanoparticles General DescriptionErbium (Er) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Erbium Particles are typically 10 - 80 nanometers (nm) with specific s.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Europium Nanoparticles General DescriptionEuropium (Eu) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Europium Particles are typically 10 - 45 nanometers (nm) with specif.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Holmium Nanoparticles General DescriptionHolmium (Ho) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 30 - 80 nanometers (nm) with speci.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Iron Cobalt Nanopowder General DescriptionIron Cobalt ( FeCo) Nanopowder or Nanoparticles, nanodots or nanocrystals are black spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Iron Nanoparticles General DescriptionIron (Fe) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Iron Particles are typically 20-40 nanometers (.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Lead Oxide Nanopowder General DescriptionLead Oxide ( PbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Lead Oxide Par.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Lithium Manganese Dioxide Nanoparticles General DescriptionLithium Manganese Oxide (LiMnO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Lithium Manganese Oxide Particles are typically 10 - 50 na.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Lithium Nanoparticles General DescriptionLithium (Li) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lithium Particles are typically 10 - 50 nanometers (nm) with specific.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Manganese Nanoparticles General DescriptionManganese (Mn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Manganese Particles are typically 20-40 na.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Nickel Nanoparticles General DescriptionNickel (Ni) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Nickel Particles are typically 10 - 40 nanometers (nm) with specific s.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Niobium Nanoparticles General DescriptionNiobium (Nb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Niobium Particles are typically 10-20 nanometers (nm) with.. |
|||
Specific Surface Area | 30 - 70 m²/g | 30 - 70 m²/g | |
American Elements Silicon Nanoparticles General DescriptionSilicon (Si) Nanoparticles, nanodots or Nanopowder are spherical high surface area metal particles. Nanoscale Silicon Particles are typically 5-25 nanometers (nm) with specific su.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Strontium Carbonate Nanoparticles General DescriptionStrontium Carbonate (SrCO3) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Strontium Carbonate Particles are typically 5 - 40 nan.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Tantalum Nanoparticles General DescriptionTantalum (Ta) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tantalum Particles are typically 10-20 nanometers (nm) wi.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Thulium Nanoparticles General DescriptionThulium (Tm) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Thulium Particles are typically 25 - 100 nanometers (nm) with specifi.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Tin Nanoparticles General DescriptionTin (Sn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tin Particles are typically 10-20 nanometers (nm) with specifi.. |
|||
Specific Surface Area | 30 - 60 m²/g | 30 - 60 m²/g | |
American Elements Ytterbium Nanoparticles General DescriptionYtterbium (Yb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Ytterbium Particles are typically 10 - 80 nanometers (nm) with spec.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Carbon Nanoparticles General DescriptionCarbon (C) Nanoparticles, nanodots or nanopowder are black spherical high surface area graphitic carbon. Nanoscale Carbon Particles are typically 10 - 45 nanometers (nm) with spec.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Cerium Nanoparticles General DescriptionCerium (Ce) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Cerium Particles are typically 5 - 40 nanometers (nm) with specific su.. |
|||
Specific Surface Area | 30 - 70 m²/g | 30 - 70 m²/g | |
American Elements Cobalt Nanoparticles General DescriptionCobalt (Co) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Cobalt Particles are typically 20-60 nanometers (nm) with specific sur.. |
|||
Specific Surface Area | 30 - 70 m²/g | 30 - 70 m²/g | |
American Elements Copper Nanoparticles General DescriptionCopper (Cu) Nanoparticles, nanodots or Nanopowder are black brown spherical high surface area metal particles. Nanoscale Copper Particles are typically 10-30 nanometers (nm) with .. |
|||
Specific Surface Area | >= 30 m²/g | >= 30 m²/g | BET |
Oceanchem Group Magnesium Hydroxide Molecular Formula: Mg(OH)2Cas No.: 1309-42-8Use: Magnesium hydroxide is a non-halogen flame retardant recommended where use of halogenated products is limited or prohibited. In addition, it is an e.. |
|||
Specific Surface Area | 30 - 50 m²/g | 30 - 50 m²/g | |
American Elements Cobalt Iron Nanopowder General DescriptionCobalt Iron ( CoFe) Nanopowder or Nanoparticles, nanodots or nanocrystals are black spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties.. |