Material Notes:
Hydraulic setting. Fine grain castable for potting and producing small tools. Used in the production of temperature probes, electrical feed-throughs, large heat treating fixtures, induction coils and crucibles. Supplied in powder form and are mixed with water to develop a strong hydraulic bond. Typically air set in 24 hours, then cured at 250 ºF for 2-4 hours to provide maximum electrical and mechanical properties.
Physical Properties Metric English Comments
Bulk Density 1.44 g/cc
0.0520 lb/in³
Powder
Open Porosity <= 6.0 %
<= 6.0 %
pH 3.0 - 4.0
3.0 - 4.0
Viscosity 16000 cP
16000 cP
Mixed. Ratio 100-to-19-22 powder-liquid
Mechanical Properties Metric English Comments
Compressive Strength 52.0 MPa
7540 psi
Thermal Properties Metric English Comments
CTE, linear 7.70 µm/m-°C

@Temperature 20.0 °C
4.28 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 17.9 W/m-K
124 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1650 °C
3000 °F
Shrinkage <= 1.0 %

@Temperature 538 °C
<= 1.0 %

@Temperature 1000 °F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
Dielectric Strength 5.90 kV/mm
150 kV/in
Processing Properties Metric English Comments
Pot Life 120 - 180 min
120 - 180 min
Shelf Life 12 Month
12 Month
Descriptive Properties Value Comments
Acid Resistance Good
Alkali Resistance Good
Color White
Moisture Resistance Good
Copyright © lookpolymers.com All Rights Reserved