Polymer Property : Melting Point = 273 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 134 °C
273 °F
Internal method
Polimeri Europa Eraclene® BB 76 High Density Polyethylene - Blow Molding
Eraclene BB 76 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 30 liters.Er..
Melting Point 134 °C
273 °F
Internal method
Polimeri Europa Eraclene® MM 74 U High Density Polyethylene - Injection Molding
Eraclene MM 74 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution. The polym..
Melting Point 134 °C
273 °F
Internal method
Polimeri Europa Eraclene® MQ 70 High Density Polyethylene - Injection Molding
Eraclene MQ 70 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MQ 70 is suggested in applications for which high creep, impact and ..
Melting Point 134 °C
273 °F
Internal method
Polimeri Europa Eraclene® MQ 74 High Density Polyethylene - Injection Molding
Eraclene MQ 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. This resin is suggested in applications for which high creep, impact and st..
Melting Point 134 °C
273 °F
Petromont
Petromont 1000 High Density Polyethylene Resin
Petromont HDPE 1000 is a high density polyethylene copolymer resin produced using the Unipol® Process. This multi-purpose resin can be used on intermittent and continuous blow moulding machines to ..
Melting Point 134 °C
273 °F
LyondellBasell Lupolen® 5261 Z HDPE, Blow Molding Grade
Relatively high viscosity blow molding grade for rigid, stackable and highly shock resistant containers for packaging all types of hazardous materials such as flammable, corrosive, poisonous and sur..
Melting Point 134 °C
273 °F
ASTM D3418
LyondellBasell Microthene® F FA70900 High Density Polyethylene
General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene..
Melting Point 134 °C
273 °F
ASTM D2117
Global B-5200 High Density Polyethylene
Description-has excellent stiffness thus requires less material to make blow moldingApplications-food containers, drinking bottles, medicine bottles, water containersInformation provided by Global ..
Melting Point 134 °C
273 °F
ASTM D2117
Global J-2208 High Density Polyethylene
Description-industrial injection grade w/ UV stabilizer, good for high impact strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided..
Melting Point 134 °C
273 °F
DSC
LG Chemical LUTENE-H BE0350 HDPE
Description: LUTENE-H BE0350 is an excellent material for blow-molded articles with high density and rigidity. It has good flow characteristics, high parison stability and impact resistance.Applicat..
Melting Point 134 - 251 °C
273 - 484 °F
Indium Corp. Indalloy 139 Lead Free Solder Alloy
Information Provided by Indium Corporation
Melting Point 134 °C
273 °F
ASTM D2117
Lushan L-5R (F) Polyethylene Copolymer Adhesive for Steel Pipe Coating
Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro..
Melting Point 134 °C
273 °F
ISO 11357
Total Lumicene® mPE M5510 EP Metallocene Polyethylene, Blown Film
This product is a Total Ecosolutions grade.Lumicene® mPE M5510 EP is a second generation metallocene high density homopolymer polyethylene.Lumicene® mPE M5510 EP can be processed at high output ra..
Melting Point 134 °C
273 °F
DSC-2 Differential Scanning Calorimeter
Total PPR 8650 Polypropylene, Random Copolymer
ATOFINA 8650 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The low melting point of ATOFINA 8650 makes it an excellent heat seal layer for orie..
Melting Point 134 °C
273 °F
ASTM D3418, ISO 3146
DuPont™ Fusabond® E100 Polymer Modifier
DuPont™ Fusabond® E100 is an anhydride modified high density polyethylene, mainly intended for use as a component in a blend with other polymers including polyolefins and polyamides. It is not int..
Melting Point 134 °C
273 °F
DSC; Dow Method
Dow DS6D81 Polypropylene Random Copolymer Resin
OverviewConsistent processabilityGood optical propertiesLow temperature heat sealComplies with U.S. FDA 21 CFR 177.1520 (c)3.1a, Canadian HPFB No ObjectionDOW DS6D81 Polypropylene Resin is intended ..
Melting Point 134 °C
273 °F
Dow Method (DSC)
Dow DS6D81 Polypropylene Resin
DOW DS6D81 is intended for use as a heat seal coating on oriented polypropylene (OPP) film.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Melting Point 134 °C
273 °F
DSC; Dow Method
Dow DS6D82 Polypropylene Random Copolymer Resin
OverviewConsistent processabilityGood optical propertiesLow temperature heat sealComplies with U.S. FDA 21 CFR 177.1520 (c)3.1aDOW DS6D82 Polypropylene Resin is intended for use as a heat seal coati..
Melting Point 134 °C
273 °F
Dow Method (DSC)
Dow DS6D82 Polypropylene Resin
DOW DS6D82 is intended for use as a heat seal coating on oriented polypropylene (OPP) film.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Melting Point 134 °C
273 °F
Dow Method (DSC)
Dow UNIVAL™ DMDC-6400 NT 7 High Density Polyethylene Resin (HDPE)
Excellent process-ability Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDC-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, wat..
Melting Point 134 °C
273 °F
DSC
Arkema Group OREVAC® 18510 Grafted Maleic Anhydride Polyethylene
OREVAC 18510 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510 is mainly used in pipe ..
Melting Point 134 °C
273 °F
DSC
Arkema Group OREVAC® 18510P Grafted Maleic Anhydride Polyethylene
OREVAC 18510P is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510P is mainly used in pip..
Melting Point 134 °C
273 °F
DSC
Arkema Group OREVAC® 18732 Grafted Maleic Anhydride Polypropylene
OREVAC 18732 and 18732P are maleic anhydride grafted polypropylene used in the manufacturing of multiplayer structures. These products are available in pellets or in powder. OREVAC 18732 and 18732P ..
Melting Point 134 °C
273 °F
DSC
Arkema Group OREVAC® 18732P Grafted Maleic Anhydride Polypropylene
OREVAC 18732 and 18732P are maleic anhydride grafted polypropylene used in the manufacturing of multiplayer structures. These products are available in pellets or in powder. OREVAC 18732 and 18732P ..
Melting Point 134 °C
273 °F
ISO 11357
Arkema Group Pebax® 2533 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 2533 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Melting Point 134 °C
273 °F
ISO 11357
Arkema Group Pebax® 2533 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 2533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Melting Point 134 °C
273 °F
ISO 11357
Arkema Group Pebax® 2533 SD 02 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 2533 SD 02 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SD grade is heat and UV stabilized and contains mold release additive.Infor..
Melting Point 134 °C
273 °F
(Dry)
Arkema Group Pebax® 2533 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 25 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness..
Melting Point 134 °C
273 °F
ISO 11357-3
Addcomp PRIEX® 12031 Maleic Anhydride Grafted HDPE
Fields of application: Functionalised polyethylene to be used as compatibiliser for polymer blends or coupling agent for wood flour, natural fibres, or mineral filled polyolefins. Also suitable to r..
Melting Point 134 °C
273 °F
Peak; ExxonMobil Method
ExxonMobil Exxelor™ PE 1040 High Density Polyethylene Resin
Product Description: Exxelor PE 1040 polymer resin is a maleic anhydride functionalized high density polyethylene, produced by reactive extrusion. It has been primarily designed to act as a coupli..