Material Notes:
Polyether block amide PEBAX® MV 1041 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on to a substrate offers excellent permeability to moisture vapor while remaining waterproof and offering an excellent barrier layer to bacteria. This SA grade is specially designed to medical and food uses.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Water Absorption 12 %
<br>@Temperature 23.0 °C,<br> Time 86400 sec
12 %
<br>@Temperature 73.4 °F,<br> Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 0.90 %
<br>@Temperature 20.0 °C
0.90 %
<br>@Temperature 68.0 °F
50% RH; ISO 62
Water Vapor Transmission 2200 g/m²/day
<br>@Thickness 0.0150 mm,<br> Temperature 38.0 °C
142 g/100 in²/day
<br>@Thickness 0.000591 in,<br> Temperature 100 °F
90% RH; ASTM E96 E
8000 g/m²/day
<br>@Thickness 0.0150 mm,<br> Temperature 38.0 °C
515 g/100 in²/day
<br>@Thickness 0.000591 in,<br> Temperature 100 °F
50% RH; ASTM E96 BW
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Instantaneous, Conditioned 15 days at 23°C - 50% RH; ISO 868
Tensile Strength at Break 44.0 MPa
6380 psi
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Elongation at Break 450 %
450 %
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Flexural Modulus 0.270 GPa
39.2 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Thermal Properties Metric English Comments
Melting Point 170 °C
338 °F
ISO 11357
Processing Properties Metric English Comments
Nozzle Temperature 190 - 210 °C
374 - 410 °F
Blown Film
240 - 250 °C
464 - 482 °F
Cast Film
240 - 250 °C
464 - 482 °F
Coating
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour