Arlon 48576R005 0.0055" (0.140 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 48576R005 0.0055" (0.140 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Cured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Side 1
>= 25.4 microns
>= 1.00 mil
Side 2
38.1 microns
1.50 mil
Polyethylene Interleave
50.8 microns
2.00 mil
Unprimed Coated 1080 Fiberglass (same as 108/no plied yarns), Substrate
63.5 microns
2.50 mil
Primed Coated 1080 Fiberglass (same as 108/no plied yarns), Substrate
114 - 165 microns
4.50 - 6.50 mil
Overall
Mechanical Properties Metric English Comments
Hardness, Shore A 40 - 50
40 - 50
Compound Property
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Elongation at Break >= 550 %
>= 550 %
Compound Property
Peel Strength >= 0.701 kN/m
>= 4.00 pli
[ppi], Bond Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
UL RTI, Electrical 220 °C
428 °F
per UL Card E54153
UL RTI, Mechanical without Impact 200 °C
392 °F
per UL Card E54153
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 177 °C
0.250 hour

@Temperature 350 °F
Recommended Cure Cycle
120 min

@Temperature 232 °C
2.00 hour

@Temperature 450 °F
Recommended Postcure Cycle
Shelf Life 6.00 Month

@Temperature <=23.9 °C
6.00 Month

@Temperature <=75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 4.5 - 5.5
Uncoated Fabric Break Strength 40 lb/in
Fill Direction, Substrate Property
70 lb/in
Warp Direction, Substrate Property