Arlon P29514R020 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon P29514R020 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassAppearance: Red silicone rubber on fiberglass fabric.This data represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInformation provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 203 microns
8.00 mil
Substrate; Arlon SQA-TMS-003
318 microns
12.5 mil
Side 1; Arlon SQA-TMS-003
521 microns
20.5 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 47
47
Silicone Property; ASTM D2240
Tensile Strength 5.17 MPa
750 psi
Silicone Property; ASTM D412
Elongation at Break 450 %
450 %
Silicone Property; ASTM D412
Peel Strength 2.02 kN/m
11.5 pli
Bond Strength; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 24.8 kV/mm
630 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 3.00 Month

@Temperature 23.9 °C
3.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 23.9