Ashley Polymers Ashlene® L925 Nylon 12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® L925 Nylon 12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. The natural color is slightly darker.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hrs; ASTM D570
Water Absorption at Saturation 1.4 %
1.4 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 49.0 MPa
7110 psi
ASTM D638
Elongation at Break 225 %
225 %
ASTM D638
Flexural Modulus 1.30 GPa
189 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
0.240 J/cm

@Temperature -40.0 °C
0.450 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 184 °C
363 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C
115 °F
ASTM D648