Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axion Polymers Axpoly® PS13 1000 Impact Modified Polystyrene

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Axion Polymers
Trade Name Axpoly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axion Polymers Axpoly® PS13 1000 Impact Modified Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PS13 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS13 range of resin compounds are processed to a high purity and give consistent material properties during injection molding and sheet extrusion.Produced from 100% post-consumer raw materials, this product fits closely with Axion's other recycled resin grades and offers the same set of user benefits, including:Successfully replaces virgin resinHuge savings in CO2 impactAppeals to 'greener' customersCost-down on raw materialInformation provided by Axion Recycling
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Typical; ISO 1183-1
1.02 - 1.06 g/cc
0.0368 - 0.0383 lb/in³
Spec; ISO 1183-1
Particle Size 2000 - 4000 µm
2000 - 4000 µm
Pellet Size
3000 µm
3000 µm
Typical
Melt Index of Compound 5.0 - 9.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 - 9.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Spec
7.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Typical
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 - 27.0 MPa
2610 - 3920 psi
Spec; ISO 527-1/2
23.0 MPa
3340 psi
Typical; ISO 527-1/2
Elongation at Break 20 - 30 %
20 - 30 %
Spec; ISO 527 - 1/2
25 %
25 %
Typical; ISO 527 - 1/2
Izod Impact, Unnotched (ISO) 6.00 - 10.0 kJ/m²
2.86 - 4.76 ft-lb/in²
Spec; ISO 180
8.00 kJ/m²
3.81 ft-lb/in²
Typical; ISO 180
Processing Properties Metric English Comments
Moisture Content 0.17 %
0.17 %
Typical
<= 0.25 %
<= 0.25 %
Spec