Electrical Properties Metric English Comments
Dielectric Strength 7.00 - 48.0 kV/mm
178 - 1220 kV/in
Average value: 28.9 kV/mm Grade Count:34
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Dielectric Strength 7.00 - 37.0 kV/mm
178 - 940 kV/in
Average value: 26.0 kV/mm Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Dielectric Strength 7.00 - 25.0 kV/mm
178 - 635 kV/in
Average value: 11.2 kV/mm Grade Count:7
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi..
Dielectric Strength 7.00 - 50.0 kV/mm
178 - 1270 kV/in
Average value: 29.0 kV/mm Grade Count:6
Overview of materials for Nylon 12, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr..
Dielectric Strength 7.00 kV/mm
178 kV/in
60°C for 500 hrs
Fujipoly Industries Sarcon® 30GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 7.00 kV/mm
178 kV/in
150°C for 1,000 hrs
Fujipoly Industries Sarcon® 30GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 7.00 kV/mm
178 kV/in
AC 60 Hz
Fujipoly Industries Sarcon® 30GSR Thin-Film GSR
Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of..
Dielectric Strength 7.00 kV/mm
178 kV/in
AC 60 Hz
Fujipoly Industries Sarcon® 30GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Strength 7.00 kV/mm
178 kV/in
AC 60 Hz; 150°C for 1,000 hrs
Fujipoly Industries Sarcon® 30H Thin-Film HR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 7.00 kV/mm
178 kV/in
200°C for 1,000 hrs
Fujipoly Industries Sarcon® 30H Thin-Film HR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 7.00 kV/mm
178 kV/in
AC 60 Hz
Fujipoly Industries Sarcon® 30Q Thin-Film QR
Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..
Dielectric Strength 7.00 kV/mm
178 kV/in
60°C for 500 hrs
Fujipoly Industries Sarcon® 45T Thin-Film TR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Strength 7.00 kV/mm
178 kV/in
LG Chemical TR557 MABS, High Transparency, High Impact
Feature: Injection Molding, High Transparency, High ImpactApplication: Electric/Electronic Applications, Copier, Printer etc.CAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical
Dielectric Strength 7.00 kV/mm
178 kV/in
AC Rapid Rise; ASTM D149
DuPont™ Nomex® N196 Paper, 5 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Dielectric Strength 7.00 kV/mm
178 kV/in
IEC 60243-1
Azoty Tarnow™ TARFLEN SM-S15G2 PTFE
Tarflen SM1 reinforced with 15% glass fibers and 2% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Dielectric Strength 7.00 - 9.00 kV/mm

@Temperature 90.0 °C
178 - 229 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R..
Dielectric Strength 7.00 - 9.00 kV/mm

@Temperature 90.0 °C
178 - 229 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa..
Dielectric Strength 7.00 - 8.00 kV/mm
178 - 203 kV/in
ASTM D149
Adamas Adalon® 453 PTFE, Mica filler
Information provided by Adamas, HPM
Dielectric Strength >= 7.00 kV/mm

@Temperature 90.0 °C
>= 178 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Good tracking resistanceGood dielectric strengthGood electrical insulation Applications:Switchgear components which ought to have high tracking resistanceCircuit protecting switche..
Dielectric Strength 7.00 - 9.00 kV/mm

@Temperature 90.0 °C
178 - 229 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R..