Car heater casings.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Linear Mold Shrinkage, Flow 0.010 cm/cm
0.010 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.0 MPa
4930 psi
Elongation at Break 3.0 %
3.0 %
Tensile Modulus 4.50 GPa
653 ksi
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
Vicat Softening Point 105 °C
221 °F