BASF Ultramid® BU50I BK 106 PA6 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer BASF
Trade Name Ultramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® BU50I BK 106 PA6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid Ultratough Nylon BU50I BK-106 is an unreinforced PA6, impact modified, pigmented black, injection molding product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme low temperature tolerance of Ultramid BU50I BK106 makes it ideal for applications in which the weld line impact strength at low temperatures is critical.Applications: Automotive components, small engines, power tool parts and casings, cold weather and high impact sports gear, such as snowboards, ski components, helmets and hockey masks.Information provided by BASF
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 2.1 %
2.1 %
50% RH; ASTM D570
7.3 %
7.3 %
Saturation; ASTM D570
Linear Mold Shrinkage 0.04572 cm/cm
0.04572 in/in
1/8" bar
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Strength 67.0 MPa
9720 psi
ASTM D790
Flexural Modulus 1.79 GPa
260 ksi
ASTM D790
Izod Impact, Notched (ISO) NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D3418
Processing Properties Metric English Comments
Melt Temperature 270 - 300 °C
518 - 572 °F
Mold Temperature 60.0 - 85.0 °C
140 - 185 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.15 %
<= 0.15 %
Descriptive Properties Value Comments
Color BK 106
Commercial Status North America