Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem H 603 Blow Molding Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Blow Molding Grade
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem H 603 Blow Molding Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: H 603 is a low melt flow rate homopolymer used for general purposes. This resin is designed for blow moulding and extrusion applications. H 603 exhibits excellent processability, excellent stiffness/impact strength balance, high melt strength and low odor/taste transfer.Applications: Bottles for mineral water, vinegar and food; Flat and corrugated sheets in general Information provided by Braskem
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792A
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Yield 33.0 MPa
4790 psi
ASTM D638
Elongation at Yield 14 %
14 %
ASTM D638
Flexural Modulus 1.35 GPa
196 ksi
1% secant; ASTM D790
Izod Impact, Notched 0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C
192 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C
127 °F
ASTM D648
Vicat Softening Point 154 °C
309 °F
10 N; ASTM D1525