CENTROPLAST CENTROFLON Polyvinylidene fluoride

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROFLON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROFLON Polyvinylidene fluoride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material has very good chemical and temperature resistance, with good slip characteristics. Its applications include pump wheels, flanges, valve bodies, and laboratory equipment.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.040 %
0.040 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 0.040 %
0.040 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75

@Thickness 10.0 mm
75

@Thickness 0.394 in
ISO 2039-2
Ball Indentation Hardness 100 MPa
14500 psi
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield 50.0 MPa
7250 psi
v = 50 mm/min; ISO 527-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2
Tensile Modulus 2.00 GPa
290 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 120 µm/m-°C

@Temperature 20.0 °C
66.7 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Melting Point 169 °C
336 °F
10K/min; ISO 3146
Maximum Service Temperature, Air 150 °C
302 °F
Long Term
160 °C
320 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
ISO 75-2
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 6.0

@Frequency 1e+6 Hz
6.0

@Frequency 1e+6 Hz
IEC 60250
7.5

@Frequency 100 Hz
7.5

@Frequency 100 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm
508 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.025

@Frequency 100 Hz
0.025

@Frequency 100 Hz
IEC 60250
0.165

@Frequency 1e+6 Hz
0.165

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Food Compliance yes
BGVV
yes