Covestro Desmopan® 3485A Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® 3485A Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extrusion- and injection molding gradesuitable for extrusion blow moldingwith release agenthigh melt stabilityApplicationBellowsInjection molded engineering partsPreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
3s; ISO 868
Hardness, Shore D 33
33
15s; ISO 868
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527-1/-2
Tensile Strength, Yield 50.0 MPa
7250 psi
parallel; ISO 527-3
5.00 MPa

@Strain 100 %
725 psi

@Strain 100 %
ISO 527-1/-2
15.0 MPa

@Strain 300 %
2180 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 25
25
mm³; ISO 4649
Compression Set 15 %

@Temperature 23.0 °C
15 %

@Temperature 73.4 °F
ISO 815
42 %

@Temperature 70.0 °C
42 %

@Temperature 158 °F
ISO 815
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America