34 Shore D, Injection Molding or Extrusion Grade
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
Water Absorption 0.75 %
0.75 %
Sim. To ISO 62
Moisture Absorption 0.300 %
0.300 %
Sim. To ISO 62
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 34

@Time 15.0 sec
34

@Time 0.00417 hour
ISO 868
Tensile Strength, Ultimate 25.0 MPa
3630 psi
ISO 527-1/-2
Tensile Stress 3.90 MPa

@Strain 10.0 %
566 psi

@Strain 10.0 %
ISO 527-1/-2
7.50 MPa

@Strain 100 %
1090 psi

@Strain 100 %
ISO 527-1/-2
Tensile Modulus 0.0500 GPa
7.25 ksi
ISO 527-1/-2
Izod Impact Resistance NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact, Notched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eA
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 220 µm/m-°C
122 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 220 µm/m-°C
122 µin/in-°F
ISO 11359-1/-2
Melting Point 195 °C
383 °F
10°C/min; ISO 11357-1/-3
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Dielectric Constant 4.0

@Frequency 1.00e+6 Hz
4.0

@Frequency 1.00e+6 Hz
IEC 60250
4.1

@Frequency 100 Hz
4.1

@Frequency 100 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm
508 kV/in
IEC 60243-1
Dissipation Factor 0.0010

@Frequency 100 Hz
0.0010

@Frequency 100 Hz
IEC 60250
0.017

@Frequency 1.00e+6 Hz
0.017

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112