Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Stanyl® 46HF5040 (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Flame Retarded + Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® 46HF5040 (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by DSM Engineering Plastics.
Physical Properties Metric English Comments
Density 1.77 g/cc
0.0639 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.3 %
1.3 %
50% RH / 23°C; Similar to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 190 MPa
27600 psi
ISO 527-1/-2
Elongation at Break 1.7 %
1.7 %
ISO 527-1/-2
Tensile Modulus 15.0 GPa
2180 ksi
ISO 527-1/-2
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179/1eU
1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 295 °C
563 °F
ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 290 °C
554 °F
ISO 75-1/-2
UL RTI, Electrical 140 °C

@Thickness 1.50 mm
284 °F

@Thickness 0.0591 in
UL746B
Flammability, UL94 V-0

@Thickness 0.350 mm
V-0

@Thickness 0.0138 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243-1
Comparative Tracking Index 350 V
350 V
IEC 60112