DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temperatures Excellent resistance to wear and low friction Outstanding flow for easy processing and exceptional design freedomStanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical propertiesKey Applications: Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensionersE&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliancesInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.77 g/cc
0.0639 lb/in³
(DAM); ISO 1183
Water Absorption 4.5 %
4.5 %
DAM; Sim. to ISO 62
Moisture Absorption at Equilibrium 1.3 %
1.3 %
Humidity Absorption (DAM); Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
DAM; ISO 294-4
0.0090 cm/cm
0.0090 in/in
DAM; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
ISO 527-1/-2
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-1/-2
Charpy Impact Unnotched 7.00 J/cm²

@Temperature 23.0 °C
33.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
1.40 J/cm²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 9500 MPa
1.38e+6 psi
ISO 899-1
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
10°C/min (DAM); ISO 11357-1/-3
UL RTI, Electrical 140 °C

@Thickness 1.50 mm
284 °F

@Thickness 0.0591 in
UL746B
140 °C

@Thickness 0.750 mm
284 °F

@Thickness 0.0295 in
UL746B
UL RTI, Mechanical with Impact 110 °C

@Thickness 0.750 mm
230 °F

@Thickness 0.0295 in
UL746B
125 °C

@Thickness 1.50 mm
257 °F

@Thickness 0.0591 in
UL746B
UL RTI, Mechanical without Impact 120 °C

@Thickness 0.750 mm
248 °F

@Thickness 0.0295 in
UL746B
125 °C

@Thickness 1.50 mm
257 °F

@Thickness 0.0591 in
UL746B
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Dielectric Strength 20.0 kV/mm
508 kV/in
IEC 60243-1
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
350 V
350 V
IEC 60112
Descriptive Properties Value Comments
Flame Retardant Yes
Flame Retarding Agent Yes
Heat stabilized or stable to heat Yes
Injection molding Yes
Lubricants Yes
Platable Yes
Release Agent Yes
With Fillers Yes
Users viewing this material also viewed the following: