Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPC-W44A Polyurethane Gel MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPC-W44A Polyurethane Gel MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-A47A Liquid Castable Polyurethane MPP-A47A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-A50A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-A60A Liquid Castable Polyurethane MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-D80B Rigid Polyurethane MPP-D80B has a high load-bearing property at hardness 80 D Durometer. This material has a relatively slow curing pattern. Whereas many polyurethane formulations of this hardness cure very fast thus.. |
|||
Processing Temperature | 21.1 - 29.4 °C | 70.0 - 85.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-F07A Easy Hand-Mixable/Pourable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing with very basic tools such as a cup and stir stick. The components are low-viscosity stable li.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-R02C Semi-rigid Polyurethane Foam Formulation MPP-R02C is semi-rigid foam formulations for molded foam products. It is closed-cell light foam with some structural integrity. Unlike rigid polyurethane foams, the physical properties of a cured pr.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-R07B Polyurethane Formulation This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is long enough to allow manual handling for cast-.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPS-F04A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPS-F08A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or machine casting by the meter dispensing equipment. The components are stable and liquid at .. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MSB-M25B Microcellular Foam based on High Performance Polyester Polyurethane This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this syste.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MSB-M25F Microcellular Foam based on High Performance Polyester Polyurethane This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this syste.. |
|||
Processing Temperature | 21.1 °C | 70.0 °F | Prepolymer Temperature |
Northstar Polymers MSS-A80AQ High Performance Polyurethane Cast Elastomer System 80A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers GK-7 Low Viscosity Polyurethane Gel Cast This material is formulated for production of thin polyurethane gel film or parts. The low viscosity property of the mixed component enables the user to cast this into a thin layer without entrappi.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MAP-R06C Semi Rigid Structural Foam Formulation MPP-R06C is a polyurethane foam formulation. It is closed-cell foam with a good structural integrity and an enhanced skin quality. Unlike polyurethane rigid foams, the physical properties of a cured.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MCG-1 OOO Scale Microcellular Gel Elastomer MCG-1 is formulated for making extremely soft products. MCG-1 has unique structure for this class of material. The cured product will be slightly foamed and give a very soft touch, yet faster resp.. |
|||
Processing Temperature | 21.1 - 35.0 °C | 70.0 - 95.0 °F | Prepolymer Temperature |
Northstar Polymers MPG-A25A Room-Temperature Curable Liquid Castable Polyurethane MPG-A25A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Processing Temperature | 21.1 - 25.0 °C | 70.0 - 77.0 °F | Prepolymer Temperature |
Northstar Polymers MPG-D70A Room-Temperature-Curable Polyurethane Casting Elastomer MPG-D70A is room-temperature-curable polyurethane casting elastomer system designed for molding polyurethane parts with tough, but flexible physical characteristics. The typical applications for th.. |
|||
Processing Temperature | 21.1 - 25.0 °C | 70.0 - 77.0 °F | Curing Agent Temperature |
Northstar Polymers MPG-D70A Room-Temperature-Curable Polyurethane Casting Elastomer MPG-D70A is room-temperature-curable polyurethane casting elastomer system designed for molding polyurethane parts with tough, but flexible physical characteristics. The typical applications for th.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers MPP-A65A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Curing Agent Temperature |
Northstar Polymers MPP-A80E High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Processing Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | Prepolymer Temperature |
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel SAI-1 is custom formulated polyurethane gel material to yield very soft elastomer gel material from low viscosity components at room temperature. This material is variable mixing ratio so that the .. |
|||
Processing Temperature | 21.1 °C | 70.0 °F | |
Devcon Backing Compound Epoxy Abrasion-Resistant SystemData provided by Ellsworth Adhesives. |
|||
Processing Temperature | 21.1 °C | 70.0 °F | |
Devcon Brushable Ceramic - Red, Blue Epoxy Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,.. |
|||
Processing Temperature | 21.1 °C | 70.0 °F | |
Devcon Plastic Steel® Putty (A) Epoxy General Repair EpoxyComments: The original metal-filled epoxy putty used for hundreds of routine maintenance, production and tooling applications. Bonds to most metal, concrete and some plastics. .. |
|||
Processing Temperature | 21.1 °C | 70.0 °F | |
Devcon Wear Guard (Fine Load) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Processing Temperature | 21.1 °C | 70.0 °F | |
Devcon Wear Guard (High Load) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Processing Temperature | 21.1 - 260 °C | 70.0 - 500 °F | Average value: 133 °C Grade Count:7 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Processing Temperature | 21.1 °C | 70.0 °F | |
Devcon Zip Patch™ Epoxy Emergency Repair ProductsComments: High-technology, adhesive-impregnated, putty patching system that cures at room temperature. Hardens to a tough, durable, waterproof finish in minutes. Easy-to-u.. |