Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 250 - 600 V | 250 - 600 V | Average value: 563 V Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Comparative Tracking Index | 150 - 600 V | 150 - 600 V | Average value: 282 V Grade Count:40 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Comparative Tracking Index | 550 - 600 V | 550 - 600 V | Average value: 575 V Grade Count:8 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL 746A |
SABIC Innovative Plastics Cycolac® BDT6500 ABS AUTOMOTIVE. Low gloss, color concentratable for interior applications. Natural only. |
|||
Comparative Tracking Index | 525 - 600 V | 525 - 600 V | Average value: 588 V Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Comparative Tracking Index | 250 - 600 V | 250 - 600 V | Average value: 464 V Grade Count:16 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Comparative Tracking Index | 100 - 600 V | 100 - 600 V | Average value: 420 V Grade Count:54 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Comparative Tracking Index | 250 - 600 V | 250 - 600 V | Average value: 456 V Grade Count:30 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Comparative Tracking Index | 500 - 600 V | 500 - 600 V | Average value: 572 V Grade Count:14 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Comparative Tracking Index | 350 - 600 V | 350 - 600 V | Average value: 522 V Grade Count:8 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Comparative Tracking Index | 425 - 600 V | 425 - 600 V | Average value: 568 V Grade Count:6 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Comparative Tracking Index | 550 - 600 V | 550 - 600 V | Average value: 596 V Grade Count:14 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Comparative Tracking Index | 175 - 600 V | 175 - 600 V | Average value: 518 V Grade Count:6 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Comparative Tracking Index | 575 - 600 V | 575 - 600 V | Average value: 589 V Grade Count:6 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
LG Chemical ALPHALAC SG910 HIPS High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
LG Chemical LUMID GP2330A(W) PA6+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Cooling Fan), E&E (Bobbin)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL Rating PLC 1 (400-600 volts) |
LG Chemical MI-750 MIPS Medium impact |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL Rating PLC 1 (400-600 volts) |
LG Chemical 92HR SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case.. |
|||
Comparative Tracking Index | 500 - 600 V | 500 - 600 V | Solution A; IEC 60112 |
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose Feature: Injection Molding, sPS+GF30%, General PurposeApplication: Pump Units, Pick-up Lends Holder, etc.CAS No. 9003-53-6 and 65997-17-3Information provided by LG Chemical |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL 746A |
SABIC Innovative Plastics NORYL SE100HX PPE+PS Improved productivity and reliability. Nonchlorinated, nonbrominated FR. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | PLC code 1; UL 746A |
SABIC Innovative Plastics Xenoy® 5220 PBT+PC (Asia Pacific) Unreinforced, polycarbonate-based polymer blend, excellent chemical resistance and impact.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | DAM; UL 746A |
DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L BK031 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
DuPont Teijin Films Mylar® EL21 Polyester Film, 1000 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
DuPont Teijin Films Mylar® LBTW Polyester Film, 75 Gauge Mylar® LBTW is an uncoated, transparent polyester film that has been corona treated on one side to provide superior wetting and adhesion of inks, primers, and adhesives. Mylar® LBTW is commerciall.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
DuPont Teijin Films Mylar® MO21 Polyester Film, 750 Gauge Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur.. |
|||
Comparative Tracking Index | 450 - 600 V | 450 - 600 V | Average value: 546 V Grade Count:6 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Comparative Tracking Index | 125 - 600 V | 125 - 600 V | Average value: 315 V Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Comparative Tracking Index | 550 - 600 V | 550 - 600 V | Average value: 556 V Grade Count:8 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |