Material Notes:
Product Description: Grilamid 2D 25 W 20 HL X black 9992 is a semi-flexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) grade. Unique properties of Grilamid 2D 25 W 20 HL X black 9992 are: High strength, high burst pressure (tube) High heat resistance Significantly lower water absorption compared to standard polyamides Good chemical and hydrolysis resistance Low density Easy processing Grilamid 2D 25 W 20 HL X black 9992 has been developed for media lines in passenger cars and trucks. Thanks to its excellent heat resistance it is particularly suitable for diesel, air brake, cooling, oil and hydraulic tubes. The product is not recommended for direct permanent contact with gasoline. One particular application is the use as outer layer of multilayer ECOSYS coolant tubes. ECOSYS (EMS Cooling System) is the designation for tube solutions developed by EMS-GRIVORY for automotive heating and cooling systems.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Water Absorption 2.1 %
2.1 %
ISO 62
Moisture Absorption 0.900 %
0.900 %
ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 30.0 MPa
4350 psi
conditioned; ISO 2039-1
39.0 MPa
5660 psi
dry; ISO 2039-1
Tensile Stress 25.0 MPa

@Strain 50.0 %
3630 psi

@Strain 50.0 %
conditioned; ISO 527-1/-2
30.0 MPa

@Strain 50.0 %
4350 psi

@Strain 50.0 %
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.380 GPa
55.1 ksi
conditioned; ISO 527-1/-2
0.550 GPa
79.8 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched NB
NB
dry; ISO 179/1eA
NB
NB
conditioned; ISO 179/1eA
1.30 J/cm²

@Temperature 30.0 °C
6.19 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 250 µm/m-°C
139 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
Melting Point 210 °C
410 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Strength 37.0 kV/mm
940 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Plasticizer
Automotive Air intake sytems
Compressed air systems
Cooling and climate control
Fuel systems
Hydraulic systems
Powertrain and Chassis
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Mechanical Engineering
Processing Other Extrusion
Profile Extrusion
Product Attributes Flexible
High viscosity
Hydrolysis resistant
Special Characteristics High impact or impact modified
Improved heat resistance
Light stabilized or stable to light
Users viewing this material also viewed the following: