EMS-Grivory Grivory® TR XE 4139 black 9231 PA*

Category Polymer , Thermoplastic , Nylon
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® TR XE 4139 black 9231 PA*.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid XE 4139 black 9231 is an amorphous thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic monomers. Grilamid XE 4139 black 9231 contains a processing aid to improve the flow- and demolding properties and is stabilized against heat aging. Grilamid XE 4139 black 9231 offers a variety of interesting properties such as: very high stiffnessgood impact performancedark black colorhigh surface hardness and glosschemical resistance especially vs. oil, grease and fuelsstress cracking resistanceimproved heat and weathering resistanceeasy processing Grilamid XE 4139 black 9231 is suitable for production of optical and technically demanding parts in the application fields of: Electrical / ElectronicsEngineering, PneumaticsAgricultureDomestic appliancesAutomotiveInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Water Absorption 7.0 %
7.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 160 MPa
23200 psi
dry; ISO 2039-1
160 MPa
23200 psi
conditioned; ISO 2039-1
Tensile Strength, Yield 95.0 MPa
13800 psi
conditioned; ISO 527-1/-2
105 MPa
15200 psi
dry; ISO 527-1/-2
Elongation at Break 25 %
25 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 6.0 %
6.0 %
conditioned; ISO 527-1/-2
7.0 %
7.0 %
dry; ISO 527-1/-2
Tensile Modulus 2.80 GPa
406 ksi
conditioned; ISO 527-1/-2
2.80 GPa
406 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
dry; ISO 179/1eA
1.20 J/cm²
5.71 ft-lb/in²
conditioned; ISO 179/1eA
1.10 J/cm²

@Temperature 30.0 °C
5.23 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
Transformation Temperature, Tg 160 °C
320 °F
10°C/min; ISO 11357-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
dry; IEC 60093
1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 27.0 kV/mm
686 kV/in
dry; IEC 60243-1
27.0 kV/mm
686 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Release agent
Automotive Fuel systems
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Mechanical Engineering
Sanitary, water and gas supply
Tools & Accessories
Processing Injection Molding
Product Attributes Barrier Properties
Co Polyamide
Hydrolysis resistant
Partially aromatic Polyamide
Transparent Polyamide
Special Characteristics Improved heat resistance
Improved UV resistance (outdoor use)
Transparent