Material Notes:
Characteristics: 20% glass fibre filled
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792, ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Index of Compound 6.0 - 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
6.0 - 10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785, ISO 2039/2
Elongation at Break 9.0 %
9.0 %
ASTM D638, ISO R527
Flexural Modulus 3.50 GPa
508 ksi
ASTM D790, ISO 178
Izod Impact, Notched >= 4.50 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 8.43 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256, ISO 180/4a
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
20000 h; VDE 0304/P2-1, IEC 216
85.0 °C
185 °F
5000 h; VDE 0304/P2-1, IEC 216
180 °C
356 °F
few hours; VDE 0304/P2-1, IEC 216
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
ASTM D648, ISO 75
Vicat Softening Point >= 110 °C

@Load 5.00 kg
>= 230 °F

@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V
>= 600 V
VDE 0303-P1, IEC 112