Material Notes:
M3019-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3019-P Has been found to exhibit good barrier properties, temperature resistance, and stress crack resistance.Information supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.932 g/cc
0.0337 lb/in³
ASTM D4883
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.3 MPa
1490 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Tensile Strength, Yield 17.2 MPa
2490 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 90 %
90 %
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Flexural Modulus 0.317 GPa
46.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 99.0 °C
210 °F
ASTM D1525