Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Voridian 800P Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Voridian 800P Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose low density formulation used for extrusion coating applications that require good stress resistance. This formula complies with FDA regulations at 21 CFR 177.1520(c)(2.1) for use in articles used for packing or holding food during cooking. Users must make their own determination that their use of this product is safe, legal, and technically suitable for their intended applications.Unless otherwise noted, all tests are run at 23°C and 50% RH.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D4883
Melt Flow 1.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 12.0 MPa
1740 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Tensile Strength, Yield 10.0 MPa
1450 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 500 %
500 %
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Flexural Modulus 0.200 GPa
29.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM D746
Descriptive Properties Value Comments
Process Extrusion Coating
Users viewing this material also viewed the following: