Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurotec® Tecomid® NB40 GR30 NL XA60 PA6, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled , Nylon 6, Glass Fiber Filled, Flame Retardant , Nylon 6, Heat Stabilized
Manufacturer Eurotec
Trade Name Tecomid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecomid® NB40 GR30 NL XA60 PA6, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Eurotec®
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Moisture Absorption 1.50 %

@Temperature 23.0 °C
1.50 %

@Temperature 73.4 °F
50% RH; ISO 960
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
Eurotec
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Eurotec
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
ISO 527
Elongation at Break 2.5 %
2.5 %
ISO 527
Tensile Modulus 9.50 GPa
1380 ksi
ISO 527
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
[10 K/min], ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75
Vicat Softening Point 210 °C

@Load 5.10 kg
410 °F

@Load 11.2 lb
ISO 306
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
Glow Wire Test 800 °C

@Thickness 2.00 mm
1470 °F

@Thickness 0.0787 in
GWIT; IEC 60695
960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
GWFI; IEC 60695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Processing Temperature 230 - 250 °C
446 - 482 °F
Feed Temperature 60.0 - 80.0 °C
140 - 176 °F
Throat
Mold Temperature 40.0 - 90.0 °C
104 - 194 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Moisture Content <= 0.20 %
<= 0.20 %
ISO 960
Hold Pressure 50.0 - 100 MPa
7250 - 14500 psi
Descriptive Properties Value Comments
Back Pressure Low
Injection Speed Medium - Fast