Eurotec® Tecomid® NB40 KK30 NL IL PA 6 30% glass fiber/mineral reinforced, impact modified, low warpage

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Eurotec
Trade Name Tecomid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecomid® NB40 KK30 NL IL PA 6 30% glass fiber/mineral reinforced, impact modified, low warpage.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good chemical resistanceGood flow and processing propertiesAPPLICATIONS: AutomotiveElectrical/ElectronicFurnitureConstructionHome appliances
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Filler Content 30 %
30 %
ISO 3451
Moisture Absorption at Equilibrium 1.8 %
1.8 %
Humidity Absorption, 50% RH, 23°C; ISO 62
Water Absorption at Saturation 5.5 %
5.5 %
23°C; ISO 62
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
ISO 527
Elongation at Break 5.0 %
5.0 %
ISO 527
Tensile Modulus 5.00 GPa
725 ksi
ISO 527
Izod Impact, Notched (ISO) 12.0 kJ/m²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
16.0 kJ/m²

@Temperature 23.0 °C
7.61 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eU
7.00 J/cm²

@Temperature 23.0 °C
33.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eA
1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
10 K/min; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
ISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
ISO 75-1/2
Vicat Softening Point 205 °C
401 °F
50N; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Glow Wire Test 650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
plaque; IEC 60695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Comparative Tracking Index 500 V
500 V
IEC 60112