ExxonMobil PP7064L1 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP7064L1 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A nucleated impact copolymer resin with medium flow, high stiffness and antistatic properties. It is suitable for molding applications like consumer products, closures, containers, toys and rigid packaging applications.Availability: Africa & Middle East and Europe Features:AntistaticGood Flow High StiffnessHigh CrystallineNucleated Uses: Construction Applications CratesIndustrial ApplicationsPails Tool/Tote BoxToysProcessing Method: Injection Molding and CompoundingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ISO 868
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527-2/50
Elongation at Yield 4.0 %
4.0 %
ISO 527-2/50
Tensile Modulus 1.60 GPa
232 ksi
Secant; ISO527-2/1
Flexural Modulus 1.50 GPa
218 ksi
ISO 178
Izod Impact, Notched (ISO) 6.09 kJ/m²
2.90 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.441 J/cm²

@Temperature -20.0 °C
2.10 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.546 J/cm²

@Temperature 0.000 °C
2.60 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
0.840 J/cm²

@Temperature 22.8 °C
4.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 324 °C
615 °F
ISO 3146
Crystallization Temperature 261 °C
502 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 53.9 °C
129 °F
ISO 75-2/A
Vicat Softening Point 148 °C
298 °F
ISO 306/A50
Users viewing this material also viewed the following: