Global ABS-1805 General Purpose ABS  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global ABS-1805 General Purpose ABS  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Flow 1.5 g/10 min
1.5 g/10 min
Cond. G; ASTM D1238
3.5 g/10 min
3.5 g/10 min
Cond. I; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength, Ultimate 42.7 MPa
6200 psi
ASTM D638
Tensile Modulus 2.45 GPa
355 ksi
ASTM D638
Flexural Yield Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in