Hyosung Topilene B240 PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Hyosung Co.
Trade Name Topilene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene B240 PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
B240 Extrusion Impact CopolymerApplications:Corrugated sheetThick sheetCharacteristics:High impactInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 0.40 g/10 min
0.40 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 65
65
ASTM D785
Tensile Strength, Yield 28.4 MPa
4120 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Izod Impact, Unnotched NB
NB
ASTM D256
0.588 J/cm

@Temperature -10.0 °C
1.10 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Vicat Softening Point 145 °C
293 °F
ASTM D1525