Ineos Nova S-7600MG Compact Polystyrene Microgranulates  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos Nova S-7600MG Compact Polystyrene Microgranulates  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact polystyrene Microgranulates, having a diameter of 0.8 -1.0 mm, especially useful for compounding and extrusion applications. Due to the very high viscosity and the absence of weakener, end-products of compounding or extruding are very hard and stiff.All mechanical properties measured under standard conditions 50% RH and 23°C.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
DIN 53479
Water Absorption <= 0.10 %
<= 0.10 %
DIN 53495
Melt Flow 2.5 g/10 min
2.5 g/10 min
DIN 53735/ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 28.0 MPa
4060 psi
DIN 53455
Elongation at Break 30 %
30 %
DIN 53455
Modulus of Elasticity 1.50 GPa
218 ksi
DIN 53457
Flexural Yield Strength 24.0 MPa
3480 psi
DIN 53452
Flexural Modulus 1.40 GPa
203 ksi
DIN 53457/ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
Low Temp; DIN 53453
8.00 kJ/m²
3.81 ft-lb/in²
DIN 53453/ISO 179
Izod Impact, Unnotched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
DIN 53752
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612
Vicat Softening Point 96.0 °C
205 °F
DIN 53460