Isoflon PEHD 500 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Isoflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PEHD 500 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
DIN 53479
Water Absorption 0.00 %
0.00 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
DIN 53505
Tensile Strength 28.0 MPa
4060 psi
DIN 53455
Elongation at Break 1200 %
1200 %
DIN 53455
Tensile Modulus 0.900 GPa
131 ksi
DIN 53457
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C
111 µin/in-°F
DIN 52328
Thermal Conductivity 0.430 W/m-K
2.98 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 135 °C
275 °F
DIN 53736
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous; DIN 52612
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
Minimum Service Temperature, Air -100 °C
-148 °F
Continuous; DIN 52612
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
DIN 53482
Dielectric Constant 2.4

@Frequency 1000 Hz
2.4

@Frequency 1000 Hz
DIN 53483
Dielectric Strength 45.0 - 90.0 kV/mm
1140 - 2290 kV/in
DIN 53481
Descriptive Properties Value Comments
Color Nat./Black
Users viewing this material also viewed the following: