Material Notes:
Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
DIN 53479
Water Absorption 0.00 %
0.00 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore D 73
73
DIN 53505
Tensile Strength 33.0 MPa
4790 psi
DIN 53455
Elongation at Break 650 %
650 %
DIN 53455
Tensile Modulus 1.30 GPa
189 ksi
DIN 53457
Thermal Properties Metric English Comments
CTE, linear 150 µm/m-°C
83.3 µin/in-°F
DIN 52328
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 160 °C
320 °F
DIN 53736
Maximum Service Temperature, Air 100 °C
212 °F
Continuous; DIN 52612
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
Minimum Service Temperature, Air -10.0 °C
14.0 °F
Continuous; DIN 52612
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
DIN 53482
Dielectric Strength 40.0 - 80.0 kV/mm
1020 - 2030 kV/in
DIN 53481
Descriptive Properties Value Comments
Color Nat./Gray
Users viewing this material also viewed the following: