Polymer Property : Tensile Strength = 4790 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 33.0 MPa
4790 psi
ASTM D638
Premix Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and ..
Tensile Strength 33.0 MPa
4790 psi
ASTM D638
Premix Premi-Glas® 3101-15 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 3101-15 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and ..
Tensile Strength 33.0 MPa
4790 psi
ASTM D638
Premix Premi-Glas® 3101-20 Polyester BMC
Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-..
Tensile Strength 33.0 MPa
4790 psi
ASTM D638
Premix Premi-Glas® 3101-22 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 3101-22 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and ..
Tensile Strength 33.0 MPa
4790 psi
ASTM D638
Premix Premi-Glas® 3101-25 Polyester BMC
Premi-Glas® 3101-25 is a 25% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL ..
Tensile Strength 33.0 MPa
4790 psi
ASTM D638
Premix Premi-Glas® 2103-10 CRSX Polyester BMC
Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U..
Tensile Strength 33.0 MPa
4790 psi
ASTM D412
GRECO ISOTHANE 3080AF Polyether TPU Resin
ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro..
Tensile Strength 33.0 MPa
4790 psi
measured on films cast from a solution in toluene; ISO 37
Kraton® D1101 A (SBS) Liner Block Copolymer
Description: Kraton D1101 A polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f..
Tensile Strength 33.0 MPa
4790 psi
measured on films cast from a solution in toluene; ISO 37
Kraton® D1101 B (SBS) Liner Block Copolymer
Description: Kraton D1101 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from South America in the physical form(s) identifi..
Tensile Strength 33.0 MPa
4790 psi
measured on films cast from a solution in toluene; ISO 37
Kraton® D1101 E (SBS) Liner Block Copolymer
Description: Kraton D1101 E polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f..
Tensile Strength 33.0 MPa
4790 psi
ISO 37
Kraton® D1101 J (SBS) Liner Block Copolymer
Description: Kraton D1101 J is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Japan in the physical form(s) outlined in the follow..
Tensile Strength 33.0 MPa
4790 psi
measured on films cast from a solution in toluene; ISO 37
Kraton® D1102 B (SBS) Liner Block Copolymer
Description: Kraton D1102 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 29.5%. It is supplied from South America in the physical form identifie..
Tensile Strength 33.0 MPa
4790 psi
measured on films cast from a solution in toluene; ISO 37
Kraton® D1102 E (SBS) Liner Block Copolymer
Description: Kraton D1102 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 28.5% mass. It is supplied from Europe in the physical form(s) identified below in..
Tensile Strength 33.0 MPa
4790 psi
ISO 37
Kraton® D1155 B (SBS) Liner Block Copolymer
Description: Kraton D1155 B is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from South America as indicated in the grade nomenclature..
Tensile Strength 33.0 MPa
4790 psi
DIN 53455
Isoflon PP Polypropylene
Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon.
Tensile Strength 33.0 MPa
4790 psi
ASTM D412
GRECO ISOTHANE 1075A Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength 33.0 MPa
4790 psi
ASTM D412
GRECO ISOTHANE 1080AF Poly(adipate)ester TPU Resin
ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject..
Tensile Strength 33.0 MPa
4790 psi
ASTM D412
GRECO ISOTHANE 2075A Poly(caprolactone)ester TPU Resin
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi..
Tensile Strength 33.0 MPa
4790 psi
measured on films cast from a solution in toluene; ISO 37
Kraton® D1102 A (SBS) Liner Block Copolymer
Description: Kraton D1102 A is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in..
Tensile Strength 33.0 MPa
4790 psi
ISO 37
Kraton® D1102 J (SBS) Liner Block Copolymer
Description: Kraton D1102 J is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Japan in the physical form(s) identified below in the..
Tensile Strength 33.0 MPa
4790 psi
ASTM D412
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
Tensile Strength 33.0 MPa

@Strain 300 %
4790 psi

@Strain 300 %
ISO 37
BASF Elastollan 1154 D FHF TPUR Flame Retardant Halogen Free
Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi..
Tensile Strength 33.0 MPa
4790 psi
50 mm/min; ISO 527-2
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures
PP-HT is a semi-crystalline plastic, with high acid and chemical resistance and mechanical strength. Due to its high resistance to temperature, PP-HT-plastics are often used in medical technology as..
Tensile Strength 33.0 MPa
4790 psi
ISO 527
Bulk Molding Compounds BMC 665 Mineral Filled, Glass Reinforced Polyester
BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good moldability, o..
Tensile Strength 33.0 MPa
4790 psi
ASTM D412
Wanhua Chemical Wanthane® WHT-1185 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.