Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 42.0 - 120 MPa | 6090 - 17400 psi | Average value: 83.0 MPa Grade Count:30 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Global N-3260 High Density Polyethylene, Yarn/Monofilament Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- ropes, fishing nets, wire & cable insulators, auto parts, pipesInformation provided by Global .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Kleerdex Vinyloy™ 100 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Utility gradeApplications: Vinyloy 100 sheet is a fire retardant that can be used to substitute effectively for ABS and other utility grade thermoplastics.Features: Vinyloy 100 sheet is a recycled g.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
KYDEX® T Acrylic/PVC Thermoplastic Sheet Impact resistant fire rated sheetApplications: External housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for equipment such as v.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
KYDEX® V Acrylic/PC Thermoplastic Sheet Utility sheetApplications: Can be used to substitute effectively for utility grade thermoplastics. It is very appropriate for hidden parts and painted parts and/or where fire retardancy is not requ.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Sumitomo Bakelite North America FM 3001 Cellulose Reinforced Phenolic Novolac FM 3001 is a self-lubricated cellulose reinforced phenolic molding compound, modified for applications requiring reduced friction and low wear. Information supplied by Sumitomo Bak North America... |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Plenco 05118-T5 Phenolic, Granular, Injection Molded PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, ve.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Plenco 1500 Polyester, Granular, Transfer Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Plenco 5118 Phenolic, Granular, Transfer Molded PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Elastomer Engineering Elastamide 200 Elastomer Modified RIM Nylon 6 26% crystallinity. Information supplied by Elastomer Engineering. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Tipco Tipcolite® THR 211 Phenolic Compound, Asbestos Wood Flour & Minerals, Soft Flow & High Electrical Properties Soft Flow Phenolic Compound, Reinforced with Asbestos Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Toyobo E2090A Thermoplastic Polyurethane Elastomer, Extrusion Grade Polycaprolactone type, featuring a good balance of mechanical strength and chemical resistance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ISO 37 |
Lubrizol ESTANE® GP72DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 72DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, TranslucentAvailable in EuropeInformati.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | DIN 53504 |
Lubrizol ESTANE® 58197 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ISO 527-1 |
Chengdu Polyster H8570 Thermoplastic Polyether-ester Elastomer (TPEE) High modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent heat-ageing resistance and toughness. Applications requiring high strength, high toughness and good .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D1708 |
DSM Biomedical BioSpan® F SPU Segmented Polyether Polyurethane (SPU) The flex life exhibited by BioSpan® SPU enables good performance in many different types of medical devices. This elastomeric polymer has shown the ability to withstand millions of flex cycles.The .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | 5 mm/min |
Arkema Group Rilsan® BMN Y BZ TL Nylon 11, Bronze Bead Filled (Dry) Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D412 |
BASF Elastollan® S95A Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D412 |
BASF Elastollan® S98A Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | |
BASF Polystyrol® 144 C Polystyrene (Europe) Very easy flowing grade, often blended with impact-modified Polystyrol or used as a coextruded glossy layer.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | 50% RH; ISO 527 |
Solvay Specialty Polymers Amodel® EXT-1800 Polyphthalamide, extrusion
(discontinued **) AMODEL EXT-1800 was developed specifically for the extrusion process. Unlike the grades targeted for injection molding, AMODEL EXT-1800 resin can be successfully extruded into tube, pipe, sheet, fil.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Kleerdex Kydex® 200 Acrylic/PVC Thermoplastic Sheet
(discontinued **) General purpose gradeApplications: Can be used to substitute effectively for both general purpose ABS and acrylic/PVC thermoplastics. Examples include data processing equipment housings, photocopy .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Kleerdex Kydex® 510 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Weatherable and decorative sheetApplications: Housings for equipment, recreation vehicles and truck parts, safety equipment, building products, signage, wall panels, facia, doors, service counters, .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Kleerdex Kydex® 550 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Weatherable monolithic sheetApplications: Housings for equipment, recreational vehicles and truck parts, safety equipment, building products, signageFeatures: Kydex 550 offers the properties of "Kyd.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Covestro Bayblend® SF 1443 Polycarbonate + ABS Blend Structural Foam
(discontinued **) Foam thickness 0.250 in. Properties values at foam density of 0.90 g/cc.Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from .. |