Kolon KOPA® KN333HFBL General Purpose Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Kolon
Trade Name Kopa®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOPA® KN333HFBL General Purpose Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Middle viscosity, flexibleApplications Band cables for vehiclesInformation provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Moisture Absorption at Equilibrium 1.43 %
1.43 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength 59.0 MPa
8560 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
Flexural Modulus 2.059 GPa
298.6 ksi
ASTM D790
Izod Impact, Notched 0.780 J/cm
1.46 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C
55.6 µin/in-°F
ASTM D696
Melting Point 255 °C
491 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.2
3.2
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Arc Resistance 115 sec
115 sec
ASTM D495
Users viewing this material also viewed the following: