Kuraray SEPTON® S2063 Thermoplastic Rubber

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Kuraray Company
Trade Name SEPTON®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray SEPTON® S2063 Thermoplastic Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhibit rubber-like properties over a wide range of temperatures. SEPTON®'s characteristics include:Excellent Mechanical PropertiesGood WeatherabilityExcellent Low Temperature PropertiesExcellent Electrical PropertiesSuperior Heat ResistanceExcellent Chemical ResistanceLow ToxicitySEPTON® grades are available with a range of Shore A hardness of 35-95 and tensile strengths of 290-5600 psi. SEPTON® resins are highly extendible with fillers, resins and oils, which allows formulation of a variety of hardness for adhesives, sealants and various compounds. As an additive, SEPTON® resins can be used to improve toughness of a variety of plastics. Several SEPTON® grades have U.S. FDA and USP Class VI approval.SEPTON® has a versatile series of grades which can be used in numerous processing techniques such as blow molding, injection molding, extrusion, hot melt and solution coatings. SEPTON® resins are thermoplastics therefore, the scrap is recyclable without significant loss of properties.Information provided by The Kuraray Group.
Physical Properties Metric English Comments
Specific Gravity 0.880 g/cc
0.880 g/cc
ISO 1183
Viscosity 29 cP

@Temperature 30.0 °C
29 cP

@Temperature 86.0 °F
10% wt, Toluene Solution
140 cP

@Temperature 30.0 °C
140 cP

@Temperature 86.0 °F
15% wt, Toluene Solution
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
22 g/10 min

@Load 10.0 kg,
Temperature 200 °C
22 g/10 min

@Load 22.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 36
36
ISO 48
Tensile Strength, Ultimate 10.8 MPa
1570 psi
ISO 37
Elongation at Break 1200 %
1200 %
100% Modulus 0.000400 GPa
0.0580 ksi
ISO 37
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+16 ohm-cm
3.00e+16 ohm-cm
measured 1 min. after applying DC 500 V; JIS K-6911
Dielectric Constant 2.31

@Frequency 50 Hz
2.31

@Frequency 50 Hz
JIS K-6911
2.31

@Frequency 1000 Hz
2.31

@Frequency 1000 Hz
JIS K-6911
2.31

@Frequency 1e+6 Hz
2.31

@Frequency 1e+6 Hz
JIS K-6911
Dielectric Strength 23.0 kV/mm
584 kV/in
Dielectric Breakdown Voltage, voltage rising rate = 1 kV/sec; JIS K-6911
Dissipation Factor 0.00020

@Frequency 50 Hz
0.00020

@Frequency 50 Hz
JIS K-6911
Dielectric Loss Index 0.00020
0.00020
10<sup>3</sup> Hz; JIS K-6911
0.00080
0.00080
10<sup>16</sup> Hz; JIS K-6911
Chemical Properties Metric English Comments
Styrene Content 13 %
13 %
Descriptive Properties Value Comments
Physical Form Pellet