Material Notes:
Linen based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many structural applications.Information provided by Aurora Technologies.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0500 lb/in³
Water Absorption 1.0 %
1.0 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 105
105
Tensile Strength, Ultimate 103 MPa
15000 psi
Flexural Strength 172 MPa
25000 psi
Compressive Strength 262 MPa
38000 psi
Shear Strength 96.5 MPa
14000 psi
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 115 °C
239 °F
Electrical
125 °C
257 °F
Mechanical
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+10 ohm-cm
7.00e+10 ohm-cm
Surface Resistance 6.00e+10 ohm
6.00e+10 ohm
Dielectric Constant 5.3

@Frequency 1e+6 Hz
5.3

@Frequency 1e+6 Hz
Dielectric Strength 13.8 kV/mm
350 kV/in
Dielectric Breakdown 70000 V
70000 V
Dissipation Factor 0.060

@Frequency 1e+6 Hz
0.060

@Frequency 1e+6 Hz
Descriptive Properties Value Comments
Color Natural/Black