Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Micropol Microlin ML27 Linear Polyethylene Rotational Molding Powder

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Manufacturer Micropol Limited
Trade Name Microlin
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Micropol Microlin ML27 Linear Polyethylene Rotational Molding Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Micropol Limited
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ASTM D792
Melt Flow 4.0 - 6.0 g/10 min
4.0 - 6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
50mm/min; ASTM D638-64T
Elongation at Break 500 %
500 %
ASTM D638-64T
Flexural Modulus 1.05 GPa
152 ksi
ASTM D760-66
Thermal Properties Metric English Comments
Vicat Softening Point 114 °C
237 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746