Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 195 °C | 383 °F | |
Multibase TPSiV® 4200-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Melt Temperature | 195 °C | 383 °F | |
Multibase TPSiV® 4200-80A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Melt Temperature | 195 - 215 °C | 383 - 419 °F | |
SABIC 118 Series Linear Low Density Polyethylene for Blown Film Product Description: 118 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. Films produced using these resins yield good tensile properties, impact st.. |
|||
Melt Temperature | 195 - 225 °C | 383 - 437 °F | |
NOVA Chemicals Novapol® HD-2007-H HDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability, very high melt strength.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provid.. |
|||
Melt Temperature | 195 - 205 °C | 383 - 401 °F | |
NOVA Chemicals Novapol® PF-0218-D Butene LLDPE Film Resin Film Properties. Features: High MI for easier extrusion.Applications: Trash bags, bags-on-roll, garment film.Data provided by the manufacturer. |
|||
Melt Temperature | 195 - 220 °C | 383 - 428 °F | |
NOVA Chemicals Novapol® PF-Y821-BP Butene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, intended for narrow die gaps.Applications: General purpose packaging, bags requiring moderate clarity, bread bags.Data provided by the m.. |
|||
Melt Temperature | 195 - 220 °C | 383 - 428 °F | |
NOVA Chemicals Novapol® PF-Y821-CP Butene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer. |
|||
Melt Temperature | 195 - 220 °C | 383 - 428 °F | |
NOVA Chemicals Novapol® TF-0119-D Hexene LLDPE Film Resin Film Properties. Features: Exceptional toughness, high strength with thin films.Applications: Thin films, premium trash bags, ice bags.Data provided by the manufacturer. |
|||
Melt Temperature | 195 - 220 °C | 383 - 428 °F | |
NOVA Chemicals Novapol® TF-0119-F Hexene LLDPE Film Resin Film Properties. Features: High strength and toughness, low gel count.Applications: Stretch wrap, blend resin.Data provided by the manufacturer. |
|||
Melt Temperature | 195 - 220 °C | 383 - 428 °F | |
NOVA Chemicals Novapol® TF-Y822-BP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness.Applications: Industrial packaging, high strength liners.Data provided by the manufacturer. |
|||
Melt Temperature | 195 - 220 °C | 383 - 428 °F | |
NOVA Chemicals Novapol® TF-Y826-CP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness, intended for narrow die gaps, high strength and toughness.Applications: Industrial bags, industrial packaging.Data provided by the manufacturer. |
|||
Melt Temperature | 195 - 220 °C | 383 - 428 °F | |
NOVA Chemicals Novapol® PF-Y821-B Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Good stiffness and machinability, good clarity with LDPE.Applications: General purpose packaging, liners.Data provided by the manufacturer. |
|||
Melt Temperature | 195 - 215 °C | 383 - 419 °F | |
LATI LASTANE 50 High Impact Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Melt Temperature | 195 - 225 °C | 383 - 437 °F | |
NOVA Chemicals Novapol® HD-2100-A MDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
Melt Temperature | 195 - 205 °C | 383 - 401 °F | |
NOVA Chemicals Novapol® PF-0118-D Butene LLDPE Film Resin Film Properties. Features: Toughness and strength, thin films.Applications: Trash bags, garment film, bags-on-roll.Data provided by the manufacturer. |
|||
Melt Temperature | 195 - 220 °C | 383 - 428 °F | |
NOVA Chemicals Novapol® PF-0118-F Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Stretch wrap, blend resin, industrial packaging.Data provided by the manufacturer. |
|||
Melt Temperature | 195 - 205 °C | 383 - 401 °F | |
NOVA Chemicals Novapol® PF-0218-B Butene Copolymer LLDPE Film Resin PF-0218-B complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Melt Temperature | 195 - 205 °C | 383 - 401 °F | |
NOVA Chemicals Novapol® PF-0218-E Butene Copolymer LLDPE Film Resin PF-0218-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Melt Temperature | 195 - 220 °C | 383 - 428 °F | |
NOVA Chemicals Novapol® TF-Y822-CP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness and machinability, exceptional toughness, suitable for narrow die gaps.Applications: Heavy duty sacks, high strength packaging.Data provided by the manufac.. |
|||
Melt Temperature | 195 - 200 °C | 383 - 392 °F | |
Borealis Borcell™ ME1244 Medium Density Polyethylene Borcell™ ME1244 is a fully formulated compound for chemical foamed telesingles. ME1244 is a medium-density polyethylene compound containing chemical blowing agent. Applications Borcell™ ME1244 i.. |
|||
Melt Temperature | 195 °C | 383 °F | Injection Molding |
Covestro Texin® 185 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialSc.. |
|||
Melt Temperature | 195 °C | 383 °F | Injection Molding |
Covestro Texin® 985U Urethane Thermoplastic Elastomer Key Features:UnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.. |
|||
Melt Temperature | 195 °C | 383 °F | Injection Molding |
Covestro Texin® 985 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer Mater.. |
|||
Melt Temperature | 195 °C | 383 °F | Optimal |
BASF Ultraform® W2320 U035 LEV POM Description: Is a POM, UV-stabilized, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF |
|||
Melt Temperature | 195 - 300 °C | 383 - 572 °F | Average value: 221 °C Grade Count:25 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m.. |
|||
Melt Temperature | 195 - 205 °C | 383 - 401 °F | Extrusion |
DuPont Performance Polymers Delrin® FG150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. It has been developed for consideration in applications and parts for th.. |
|||
Melt Temperature | 195 - 302 °C | 383 - 576 °F | Average value: 232 °C Grade Count:3 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |
|||
Melt Temperature | 195 - 220 °C | 383 - 428 °F | |
NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin
(discontinued **) Film Properties. Features: Good stiffness and machinability, intended for narrow die gaps, high strength and toughness.Applications: Grocery sacks, boutique bags, frozen food packaging.Data provide.. |