Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 8.30 MPa | 1200 psi | ASTM D 882 |
NOVA Chemicals Sclair® FP619-A Octene Copolymer LLDPE Film Resin FP619-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, withou.. |
|||
Film Tensile Strength at Yield, TD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1018 DA Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Yield, TD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1018 FA Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Yield, TD | 8.30 MPa | 1200 psi | ASTM D882 |
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Film Tensile Strength at Yield, TD | 8.30 MPa | 1200 psi | ASTM D882 |
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera.. |
|||
Film Tensile Strength at Yield, TD | 8.30 MPa | 1200 psi | ASTM D882 |
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Film Tensile Strength at Yield, TD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 141.87 Shrink Film Resin LD 141.87 is a vinyl acetate copolymer film resin with very good toughness and shrink properties. Applications include Medium duty shrink wrap and Heavy duty bags.Information provided by ExxonMobil.. |
|||
Film Tensile Strength at Yield, TD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil LDPE LD 313.NF Low Density Polyethylene Resin Product Description: LD 313.NF is a 3 % vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopoly.. |
|||
Film Tensile Strength at Yield, TD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002.09 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Film Tensile Strength at Yield, TD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Film Tensile Strength at Yield, TD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Film Tensile Strength at Yield, TD | 8.30 MPa | 1200 psi | |
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u.. |
|||
Film Tensile Strength at Yield, TD | 8.30 MPa | 1200 psi | |
Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer Next Generation DOWLEX® NG 3347A resin with extra stretch performance (ESP)is an ethylene-octene-1 copolymer designed for cast stretch film applications such as industrial pallet wrap. DOWLEX NG 33.. |
|||
Film Tensile Strength at Yield, TD | 8.27 MPa | 1200 psi | ASTM D882 |
Dow INTEGRAL™ 917 Monolayer Bonding Film INTEGRAL 917 Adhesive Film is a single layer adhesive film for use where a higher flow rate and lower melt point are required. It is useful for bonding heat sensitive materials, or for porous subst.. |
|||
Film Tensile Strength at Yield, TD | 8.30 MPa | 1200 psi | |
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Film Tensile Strength at Yield, TD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1018 EA Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Film Tensile Strength at Yield, TD | 8.30 - 12.0 MPa | 1200 - 1740 psi | Average value: 9.92 MPa Grade Count:28 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum.. |
|||
Film Tensile Strength at Yield, TD | 8.27 MPa | 1200 psi | ASTM D882 |
ExxonMobil Exceed™ 1015HA Metallocene Polyethylene Resin Product Description: Exceed 1015 mVLDPE resin is metallocene ethylene-hexene copolymer. Films made from Exceed 1015 mVLDPE have outstanding cold temperature toughness, impact strength and puncture. .. |
|||
Film Tensile Strength at Yield, TD | 8.27 MPa | 1200 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1018 EB Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |