Okulen® 500 PE-HMW, Coloured

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Okulen
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Okulen® 500 PE-HMW, Coloured.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excellent job with its impact strength and insulating properties.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ISO 1183-A
Water Absorption <= 0.10 %
<= 0.10 %
Mechanical Properties Metric English Comments
Hardness, Shore D 65

@Thickness 5.00 mm
65

@Thickness 0.197 in
3 s value; plate; ISO 868
Tensile Strength, Yield 20.0 - 26.0 MPa
2900 - 3770 psi
50 mm/min; ISO/R 527
Elongation at Break >= 50 %
>= 50 %
50 mm/min; ISO/R 527
Creep Strength 10.0 MPa

@Temperature 20.0 °C,
Time 605000 sec
1450 psi

@Temperature 68.0 °F,
Time 168 hour
Charpy Impact Unnotched 1.00 - 2.00 J/cm²
4.76 - 9.52 ft-lb/in²
ISO 11542-2
Coefficient of Friction, Dynamic 0.20

@Pressure 2.00 MPa
0.20

@Pressure 290 psi
PE-metal, V = 10 m/min; ASTM D1894
Abrasion 400
400
Slurry-Test rel to GUR 4120 = 100%; DIN 58836
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C
111 µin/in-°F
DIN 53752
Melting Point 130 - 135 °C
266 - 275 °F
DSC ISO 3146
Maximum Service Temperature, Air 80.0 °C
176 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 1.00e+14 ohm-cm
<= 1.00e+14 ohm-cm
Teil 30; IEC 600093 / VDE 0303
Surface Resistance <= 1.00e+13 ohm
<= 1.00e+13 ohm
Teil 30; IEC 60093 / VDE 0303