P & P Technology KE Series Cored Shielding Mesh Gasket Strip

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer P & P Technology
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF P & P Technology KE Series Cored Shielding Mesh Gasket Strip.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cover: Knitted Monel To BS 3075-NA 13 0.11mm Dia 2 Layers. Core Material: Neoprene closed cell sponge.Information provided by P & P Technology
Physical Properties Metric English Comments
Specific Gravity 0.150 - 0.210 g/cc
0.150 - 0.210 g/cc
Water Absorption 0.70 %
0.70 %
core
Mechanical Properties Metric English Comments
Hardness, Shore A 38 - 55
38 - 55
Compression Set 17 %

@Time 86400 sec
17 %

@Time 24.0 hour
50% compression
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
Minimum Service Temperature, Air -38.0 °C
-36.4 °F
Electrical Properties Metric English Comments
Shielding Effectiveness 285 dB
285 dB
To Mil Stn
45 dB

@Frequency 10000 Hz
45 dB

@Frequency 10000 Hz
H-Field
49 dB

@Frequency 100000 Hz
49 dB

@Frequency 100000 Hz
H-Field
60 dB

@Frequency 1.00e+6 Hz
60 dB

@Frequency 1.00e+6 Hz
H-Field
75 dB

@Frequency 1.00e+10 Hz
75 dB

@Frequency 1.00e+10 Hz
P-Field
89 dB

@Frequency 1.00e+9 Hz
89 dB

@Frequency 1.00e+9 Hz
P-Field
>= 100 dB

@Frequency 1.00e+6 Hz
>= 100 dB

@Frequency 1.00e+6 Hz
E-Field
>= 100 dB

@Frequency 1.00e+7 Hz
>= 100 dB

@Frequency 1.00e+7 Hz
E-Field
>= 100 dB

@Frequency 1.00e+7 Hz
>= 100 dB

@Frequency 1.00e+7 Hz
E-Field
Descriptive Properties Value Comments
Color Black