Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PBI Performance Products Celazole® TF-60 C Carbon Fiber Reinforced Melt Processable Polybenzimidazole

Category Polymer , Thermoplastic , Polybenzimidazole (PBI)
Manufacturer PBI Performance Products, Inc.
Trade Name Celazole®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PBI Performance Products Celazole® TF-60 C Carbon Fiber Reinforced Melt Processable Polybenzimidazole.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. Celazole® T-Series products combine the superior mechanical properties and thermal resistance of PBI with the melt process ability of polyaryletherketones.Designed for injection molding and extrusionTF-60C is a carbon-reinforced blend, ideal for parts that require high strength, very low creep, and deflection resistance. A great match for planetary gears, office equipment, semiconductor, electronic and mechanical applications.Information provided by PBI Performance Products
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
Water Absorption 0.15 %

@Temperature 22.8 °C,
Time 86400 sec
0.15 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Moisture Absorption at Equilibrium 4.0 %
4.0 %
ASTM D570
Loss On Ignition 5.0 %

@Temperature 599 °C
5.0 %

@Temperature 1110 °F
Air; ASTM TGA
5.0 %

@Temperature 627 °C
5.0 %

@Temperature 1160 °F
Nitrogen; ASTM TGA
Mechanical Properties Metric English Comments
Hardness, Rockwell A 30
30
ASTM D785
Tensile Strength 230 MPa
33400 psi
ASTM D638
Elongation at Break 1.4 %
1.4 %
Tensile Modulus 24.0 GPa
3480 ksi
Flexural Strength 320 MPa
46400 psi
ASTM D790
Flexural Modulus 21.0 GPa
3050 ksi
Compressive Strength 220 MPa
31900 psi
ASTM D695
Compressive Modulus 3.80 GPa
551 ksi
Poissons Ratio 0.39
0.39
Shear Modulus 8.63 GPa
1250 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 26.0 µm/m-°C

@Temperature 25.0 - 150 °C
14.4 µin/in-°F

@Temperature 77.0 - 302 °F
ASTM TMA
Specific Heat Capacity 1.17 J/g-°C

@Temperature 70.0 °C
0.280 BTU/lb-°F

@Temperature 158 °F
ASTM D648
Thermal Conductivity 0.447 W/m-K

@Temperature 23.9 °C
3.10 BTU-in/hr-ft²-°F

@Temperature 75.0 °F
ASTM F-433
Deflection Temperature at 1.8 MPa (264 psi) 320 °C
608 °F
ASTM D648