Plastcom SLOVALEN PH 59 GF 30 PP, 30% glass fibre

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PH 59 GF 30 PP, 30% glass fibre.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suitable for automotive, engineering, electrical and consumer goods industry. With the increasing content of GF also the toughness, tensile and bending strength, modulus in tension and bending increase and the shrinkage decreases as well as the heat application increases up to 150°C. Additional drying of the material is not necessary. Delivered in natural mode and in the full RAL colour scale. Production of the fuel tank caps for the transport vehicles, shells for the textile industry.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Linear Mold Shrinkage 0.0072 cm/cm
0.0072 in/in
Linear Mold Shrinkage, Transverse 0.0082 cm/cm
0.0082 in/in
Melt Flow 6.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
6.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
Elongation at Break 30 %
30 %
Tensile Modulus 5.65 GPa
819 ksi
Flexural Strength 128 MPa
18600 psi
Flexural Modulus 4.89 GPa
709 ksi
Charpy Impact Unnotched 4.50 J/cm²

@Temperature -20.0 °C
21.4 ft-lb/in²

@Temperature -4.00 °F
5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.900 J/cm²

@Temperature -20.0 °C
4.28 ft-lb/in²

@Temperature -4.00 °F
1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 134 °C
273 °F
Vicat Softening Point 162 °C
324 °F
B
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 hour
2 hour
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi
Users viewing this material also viewed the following: